Resumo: | The hydrogen absorption and desorption of Ti53Zr27Ni20 icosahedral quasicrystal (ICQ) and Ti50Ni50 shape memory alloy (SMA) melt-spun ribbons was studied. Samples were exposed to hydrogen gas at 623 K and 4 MPa for 1000 minutes. The total capacity of hydrogen obtained for Ti53Zr27Ni20 and Ti50Ni50 was 3.2 and 2.4 wt. % respectively. The Thermal Desorption Spectrometry (TDS) of the hydrogenated alloys shows that both alloys start to desorb hydrogen around 750 K. X-ray diffraction (XRD) patterns, performed after hydrogenation, indicate a complete amorphization of the Ti53Zr27Ni20 i-phase alloy, while the Ti50Ni50 alloy remained crystalline after hydride formation. |
id |
ABMABCABPOL-1_d4344f53689c44c4528edc10b3e892dd |
---|---|
oai_identifier_str |
oai:scielo:S1516-14392013000300022 |
network_acronym_str |
ABMABCABPOL-1 |
network_name_str |
Materials research (São Carlos. Online) |
repository_id_str |
|
spelling |
Hydrogen absorption study of ti-based alloys performed by melt-spinninghydrogen absorptionTi-Ni alloyTi-Zr-Ni alloyThe hydrogen absorption and desorption of Ti53Zr27Ni20 icosahedral quasicrystal (ICQ) and Ti50Ni50 shape memory alloy (SMA) melt-spun ribbons was studied. Samples were exposed to hydrogen gas at 623 K and 4 MPa for 1000 minutes. The total capacity of hydrogen obtained for Ti53Zr27Ni20 and Ti50Ni50 was 3.2 and 2.4 wt. % respectively. The Thermal Desorption Spectrometry (TDS) of the hydrogenated alloys shows that both alloys start to desorb hydrogen around 750 K. X-ray diffraction (XRD) patterns, performed after hydrogenation, indicate a complete amorphization of the Ti53Zr27Ni20 i-phase alloy, while the Ti50Ni50 alloy remained crystalline after hydride formation.ABM, ABC, ABPol2013-06-01info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersiontext/htmlhttp://old.scielo.br/scielo.php?script=sci_arttext&pid=S1516-14392013000300022Materials Research v.16 n.3 2013reponame:Materials research (São Carlos. Online)instname:Universidade Federal de São Carlos (UFSCAR)instacron:ABM ABC ABPOL10.1590/S1516-14392013005000049info:eu-repo/semantics/openAccessRibeiro,R.M.Lemus,L.F.Santos,D.S. doseng2013-06-04T00:00:00Zoai:scielo:S1516-14392013000300022Revistahttp://www.scielo.br/mrPUBhttps://old.scielo.br/oai/scielo-oai.phpdedz@power.ufscar.br1980-53731516-1439opendoar:2013-06-04T00:00Materials research (São Carlos. Online) - Universidade Federal de São Carlos (UFSCAR)false |
dc.title.none.fl_str_mv |
Hydrogen absorption study of ti-based alloys performed by melt-spinning |
title |
Hydrogen absorption study of ti-based alloys performed by melt-spinning |
spellingShingle |
Hydrogen absorption study of ti-based alloys performed by melt-spinning Ribeiro,R.M. hydrogen absorption Ti-Ni alloy Ti-Zr-Ni alloy |
title_short |
Hydrogen absorption study of ti-based alloys performed by melt-spinning |
title_full |
Hydrogen absorption study of ti-based alloys performed by melt-spinning |
title_fullStr |
Hydrogen absorption study of ti-based alloys performed by melt-spinning |
title_full_unstemmed |
Hydrogen absorption study of ti-based alloys performed by melt-spinning |
title_sort |
Hydrogen absorption study of ti-based alloys performed by melt-spinning |
author |
Ribeiro,R.M. |
author_facet |
Ribeiro,R.M. Lemus,L.F. Santos,D.S. dos |
author_role |
author |
author2 |
Lemus,L.F. Santos,D.S. dos |
author2_role |
author author |
dc.contributor.author.fl_str_mv |
Ribeiro,R.M. Lemus,L.F. Santos,D.S. dos |
dc.subject.por.fl_str_mv |
hydrogen absorption Ti-Ni alloy Ti-Zr-Ni alloy |
topic |
hydrogen absorption Ti-Ni alloy Ti-Zr-Ni alloy |
description |
The hydrogen absorption and desorption of Ti53Zr27Ni20 icosahedral quasicrystal (ICQ) and Ti50Ni50 shape memory alloy (SMA) melt-spun ribbons was studied. Samples were exposed to hydrogen gas at 623 K and 4 MPa for 1000 minutes. The total capacity of hydrogen obtained for Ti53Zr27Ni20 and Ti50Ni50 was 3.2 and 2.4 wt. % respectively. The Thermal Desorption Spectrometry (TDS) of the hydrogenated alloys shows that both alloys start to desorb hydrogen around 750 K. X-ray diffraction (XRD) patterns, performed after hydrogenation, indicate a complete amorphization of the Ti53Zr27Ni20 i-phase alloy, while the Ti50Ni50 alloy remained crystalline after hydride formation. |
publishDate |
2013 |
dc.date.none.fl_str_mv |
2013-06-01 |
dc.type.driver.fl_str_mv |
info:eu-repo/semantics/article |
dc.type.status.fl_str_mv |
info:eu-repo/semantics/publishedVersion |
format |
article |
status_str |
publishedVersion |
dc.identifier.uri.fl_str_mv |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1516-14392013000300022 |
url |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1516-14392013000300022 |
dc.language.iso.fl_str_mv |
eng |
language |
eng |
dc.relation.none.fl_str_mv |
10.1590/S1516-14392013005000049 |
dc.rights.driver.fl_str_mv |
info:eu-repo/semantics/openAccess |
eu_rights_str_mv |
openAccess |
dc.format.none.fl_str_mv |
text/html |
dc.publisher.none.fl_str_mv |
ABM, ABC, ABPol |
publisher.none.fl_str_mv |
ABM, ABC, ABPol |
dc.source.none.fl_str_mv |
Materials Research v.16 n.3 2013 reponame:Materials research (São Carlos. Online) instname:Universidade Federal de São Carlos (UFSCAR) instacron:ABM ABC ABPOL |
instname_str |
Universidade Federal de São Carlos (UFSCAR) |
instacron_str |
ABM ABC ABPOL |
institution |
ABM ABC ABPOL |
reponame_str |
Materials research (São Carlos. Online) |
collection |
Materials research (São Carlos. Online) |
repository.name.fl_str_mv |
Materials research (São Carlos. Online) - Universidade Federal de São Carlos (UFSCAR) |
repository.mail.fl_str_mv |
dedz@power.ufscar.br |
_version_ |
1754212662878666752 |