Resumo: | Abstract This article evaluates the efficiency, benefits and limitations of pre-concentration by density separation for process mineralogy studies of low-grade gold ore. The pre-concentration by density aims to generate a product with a high content of gold and to maximize the number of gold-bearing particles characterized, thereby increasing the representativity and reducing the number of polished sections to be analyzed. Pre-concentration by density was carried out for a low-grade sulfide gold ore (0.96 ppm) from the north of Brazil. The sample was ground to below 1.7 mm, sieved down to 0.037 mm and subjected to density separation, amalgamation of the heavy product and cyanide leaching of all products. Gold was assessed in each product to evaluate the separation recovery and distribution. The finer the particle size, the higher the gold distribution in the heavy product, due to a higher degree of liberation of gold and sulfides; these values varied from 65% to 84% in fractions below 0.60 mm and decreased from 40% to 13% in the coarser fractions. Regarding gold distribution, fractions finer than 0.84 mm indicates a notable increase on gold recovery by amalgamation, indication higher surface exposure. |
id |
FG-1_67fd01d0113a82d1b777e6c7970574f2 |
---|---|
oai_identifier_str |
oai:scielo:S2448-167X2020000400579 |
network_acronym_str |
FG-1 |
network_name_str |
REM - International Engineering Journal |
repository_id_str |
|
spelling |
Effective density concentration in refractory gold ore for characterization purposespre-concentrationgold orecyanidation and amalgamationAbstract This article evaluates the efficiency, benefits and limitations of pre-concentration by density separation for process mineralogy studies of low-grade gold ore. The pre-concentration by density aims to generate a product with a high content of gold and to maximize the number of gold-bearing particles characterized, thereby increasing the representativity and reducing the number of polished sections to be analyzed. Pre-concentration by density was carried out for a low-grade sulfide gold ore (0.96 ppm) from the north of Brazil. The sample was ground to below 1.7 mm, sieved down to 0.037 mm and subjected to density separation, amalgamation of the heavy product and cyanide leaching of all products. Gold was assessed in each product to evaluate the separation recovery and distribution. The finer the particle size, the higher the gold distribution in the heavy product, due to a higher degree of liberation of gold and sulfides; these values varied from 65% to 84% in fractions below 0.60 mm and decreased from 40% to 13% in the coarser fractions. Regarding gold distribution, fractions finer than 0.84 mm indicates a notable increase on gold recovery by amalgamation, indication higher surface exposure.Fundação Gorceix2020-12-01info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersiontext/htmlhttp://old.scielo.br/scielo.php?script=sci_arttext&pid=S2448-167X2020000400579REM - International Engineering Journal v.73 n.4 2020reponame:REM - International Engineering Journalinstname:Fundação Gorceix (FG)instacron:FG10.1590/0370-44672020730031info:eu-repo/semantics/openAccessCosta,Fabrizzio RodriguesNery,Guilherme PinhoAntoniassi,Juliana LíviUlsen,Carinaeng2020-09-28T00:00:00Zoai:scielo:S2448-167X2020000400579Revistahttps://www.rem.com.br/?lang=pt-brPRIhttps://old.scielo.br/oai/scielo-oai.php||editor@rem.com.br2448-167X2448-167Xopendoar:2020-09-28T00:00REM - International Engineering Journal - Fundação Gorceix (FG)false |
dc.title.none.fl_str_mv |
Effective density concentration in refractory gold ore for characterization purposes |
title |
Effective density concentration in refractory gold ore for characterization purposes |
spellingShingle |
Effective density concentration in refractory gold ore for characterization purposes Costa,Fabrizzio Rodrigues pre-concentration gold ore cyanidation and amalgamation |
title_short |
Effective density concentration in refractory gold ore for characterization purposes |
title_full |
Effective density concentration in refractory gold ore for characterization purposes |
title_fullStr |
Effective density concentration in refractory gold ore for characterization purposes |
title_full_unstemmed |
Effective density concentration in refractory gold ore for characterization purposes |
title_sort |
Effective density concentration in refractory gold ore for characterization purposes |
author |
Costa,Fabrizzio Rodrigues |
author_facet |
Costa,Fabrizzio Rodrigues Nery,Guilherme Pinho Antoniassi,Juliana Lívi Ulsen,Carina |
author_role |
author |
author2 |
Nery,Guilherme Pinho Antoniassi,Juliana Lívi Ulsen,Carina |
author2_role |
author author author |
dc.contributor.author.fl_str_mv |
Costa,Fabrizzio Rodrigues Nery,Guilherme Pinho Antoniassi,Juliana Lívi Ulsen,Carina |
dc.subject.por.fl_str_mv |
pre-concentration gold ore cyanidation and amalgamation |
topic |
pre-concentration gold ore cyanidation and amalgamation |
description |
Abstract This article evaluates the efficiency, benefits and limitations of pre-concentration by density separation for process mineralogy studies of low-grade gold ore. The pre-concentration by density aims to generate a product with a high content of gold and to maximize the number of gold-bearing particles characterized, thereby increasing the representativity and reducing the number of polished sections to be analyzed. Pre-concentration by density was carried out for a low-grade sulfide gold ore (0.96 ppm) from the north of Brazil. The sample was ground to below 1.7 mm, sieved down to 0.037 mm and subjected to density separation, amalgamation of the heavy product and cyanide leaching of all products. Gold was assessed in each product to evaluate the separation recovery and distribution. The finer the particle size, the higher the gold distribution in the heavy product, due to a higher degree of liberation of gold and sulfides; these values varied from 65% to 84% in fractions below 0.60 mm and decreased from 40% to 13% in the coarser fractions. Regarding gold distribution, fractions finer than 0.84 mm indicates a notable increase on gold recovery by amalgamation, indication higher surface exposure. |
publishDate |
2020 |
dc.date.none.fl_str_mv |
2020-12-01 |
dc.type.driver.fl_str_mv |
info:eu-repo/semantics/article |
dc.type.status.fl_str_mv |
info:eu-repo/semantics/publishedVersion |
format |
article |
status_str |
publishedVersion |
dc.identifier.uri.fl_str_mv |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S2448-167X2020000400579 |
url |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S2448-167X2020000400579 |
dc.language.iso.fl_str_mv |
eng |
language |
eng |
dc.relation.none.fl_str_mv |
10.1590/0370-44672020730031 |
dc.rights.driver.fl_str_mv |
info:eu-repo/semantics/openAccess |
eu_rights_str_mv |
openAccess |
dc.format.none.fl_str_mv |
text/html |
dc.publisher.none.fl_str_mv |
Fundação Gorceix |
publisher.none.fl_str_mv |
Fundação Gorceix |
dc.source.none.fl_str_mv |
REM - International Engineering Journal v.73 n.4 2020 reponame:REM - International Engineering Journal instname:Fundação Gorceix (FG) instacron:FG |
instname_str |
Fundação Gorceix (FG) |
instacron_str |
FG |
institution |
FG |
reponame_str |
REM - International Engineering Journal |
collection |
REM - International Engineering Journal |
repository.name.fl_str_mv |
REM - International Engineering Journal - Fundação Gorceix (FG) |
repository.mail.fl_str_mv |
||editor@rem.com.br |
_version_ |
1754734691846455296 |