Effect of Hydrofluoric Acid Concentration and Thermal Cycling on the Bond Strength of Brackets to Ceramic
Autor(a) principal: | |
---|---|
Data de Publicação: | 2019 |
Outros Autores: | , , , , , , |
Tipo de documento: | Artigo |
Idioma: | eng |
Título da fonte: | Brazilian Dental Journal |
Texto Completo: | http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0103-64402019000600587 |
Resumo: | Abstract This study to evaluate the effects of different hydrofluoric acid (HF) concentrations and thermal cycling on the shear bond strength (SBS) of brackets to ceramic. Cylinders of ceramic were divided into 10 groups (n=15), according to HF concentrations: 1-1%;2-2.5%;3-5%;4-7.5%;5-10% (storage 24 h); 6-1%;7-2.5%;8-5%;9-7.5%; and, 10-10% (thermal cycling). All cylinders were etched for 60s and received one layer of silane. Metallic brackets were bonded to the cylinders using Transbond-XT, light activated for 40 s, using a LED (Radii Plus) and stored in deionized water at 37o C for 24h. The groups 6 to 10 were submitted to thermal cycling (7,000 cycles - 5o/55oC). SBS was performed in an Instron at crosshead speed of 1.0 mm/min. Data were submitted to two-way ANOVA and Tukey’s post-hoc test (α=0.05). The Adhesive Remaining Index (ARI) was evaluated at 40x magnification. The different HF acid concentrations influenced on the SBS of the brackets to ceramic (p<0.05). The thermal cycling decreased the SBS of the brackets to ceramic for all acid concentrations (p<0.05). The ARI showed a predominance of scores 0 for all groups, with an increase in scores 1, 2 and 3 for the group storage for 24 h. In conclusion, the different HF acid concentrations 5.0%, 7.5% and 10% influenced on the SBS of brackets to ceramic. The thermal cycling decreased significantly the SBS of brackets to ceramic. |
id |
FUNORP-1_f2cc1aa7fa0c53518053d943267054c4 |
---|---|
oai_identifier_str |
oai:scielo:S0103-64402019000600587 |
network_acronym_str |
FUNORP-1 |
network_name_str |
Brazilian Dental Journal |
repository_id_str |
|
spelling |
Effect of Hydrofluoric Acid Concentration and Thermal Cycling on the Bond Strength of Brackets to Ceramicceramicdental materialshydrofluoric acidthermal cyclingorthodonticAbstract This study to evaluate the effects of different hydrofluoric acid (HF) concentrations and thermal cycling on the shear bond strength (SBS) of brackets to ceramic. Cylinders of ceramic were divided into 10 groups (n=15), according to HF concentrations: 1-1%;2-2.5%;3-5%;4-7.5%;5-10% (storage 24 h); 6-1%;7-2.5%;8-5%;9-7.5%; and, 10-10% (thermal cycling). All cylinders were etched for 60s and received one layer of silane. Metallic brackets were bonded to the cylinders using Transbond-XT, light activated for 40 s, using a LED (Radii Plus) and stored in deionized water at 37o C for 24h. The groups 6 to 10 were submitted to thermal cycling (7,000 cycles - 5o/55oC). SBS was performed in an Instron at crosshead speed of 1.0 mm/min. Data were submitted to two-way ANOVA and Tukey’s post-hoc test (α=0.05). The Adhesive Remaining Index (ARI) was evaluated at 40x magnification. The different HF acid concentrations influenced on the SBS of the brackets to ceramic (p<0.05). The thermal cycling decreased the SBS of the brackets to ceramic for all acid concentrations (p<0.05). The ARI showed a predominance of scores 0 for all groups, with an increase in scores 1, 2 and 3 for the group storage for 24 h. In conclusion, the different HF acid concentrations 5.0%, 7.5% and 10% influenced on the SBS of brackets to ceramic. The thermal cycling decreased significantly the SBS of brackets to ceramic.Fundação Odontológica de Ribeirão Preto2019-11-01info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersiontext/htmlhttp://old.scielo.br/scielo.php?script=sci_arttext&pid=S0103-64402019000600587Brazilian Dental Journal v.30 n.6 2019reponame:Brazilian Dental Journalinstname:Fundação Odontológica de Ribeirão Preto (FUNORP)instacron:FUNORP10.1590/0103-6440201902989info:eu-repo/semantics/openAccessAguiar,Ana PaulaCosta,Ana RosaCorrer,Américo BortolazzoVedovello,Silvia AméliaVedovello Filho,MárioCrepaldi,Marcus ViniciusValdrighi,Heloísa CristinaCorrer-Sobrinho,Lourençoeng2019-11-25T00:00:00Zoai:scielo:S0103-64402019000600587Revistahttps://www.scielo.br/j/bdj/https://old.scielo.br/oai/scielo-oai.phpbdj@forp.usp.br||sergio@fosjc.unesp.br1806-47600103-6440opendoar:2019-11-25T00:00Brazilian Dental Journal - Fundação Odontológica de Ribeirão Preto (FUNORP)false |
dc.title.none.fl_str_mv |
Effect of Hydrofluoric Acid Concentration and Thermal Cycling on the Bond Strength of Brackets to Ceramic |
title |
Effect of Hydrofluoric Acid Concentration and Thermal Cycling on the Bond Strength of Brackets to Ceramic |
spellingShingle |
Effect of Hydrofluoric Acid Concentration and Thermal Cycling on the Bond Strength of Brackets to Ceramic Aguiar,Ana Paula ceramic dental materials hydrofluoric acid thermal cycling orthodontic |
title_short |
Effect of Hydrofluoric Acid Concentration and Thermal Cycling on the Bond Strength of Brackets to Ceramic |
title_full |
Effect of Hydrofluoric Acid Concentration and Thermal Cycling on the Bond Strength of Brackets to Ceramic |
title_fullStr |
Effect of Hydrofluoric Acid Concentration and Thermal Cycling on the Bond Strength of Brackets to Ceramic |
title_full_unstemmed |
Effect of Hydrofluoric Acid Concentration and Thermal Cycling on the Bond Strength of Brackets to Ceramic |
title_sort |
Effect of Hydrofluoric Acid Concentration and Thermal Cycling on the Bond Strength of Brackets to Ceramic |
author |
Aguiar,Ana Paula |
author_facet |
Aguiar,Ana Paula Costa,Ana Rosa Correr,Américo Bortolazzo Vedovello,Silvia Amélia Vedovello Filho,Mário Crepaldi,Marcus Vinicius Valdrighi,Heloísa Cristina Correr-Sobrinho,Lourenço |
author_role |
author |
author2 |
Costa,Ana Rosa Correr,Américo Bortolazzo Vedovello,Silvia Amélia Vedovello Filho,Mário Crepaldi,Marcus Vinicius Valdrighi,Heloísa Cristina Correr-Sobrinho,Lourenço |
author2_role |
author author author author author author author |
dc.contributor.author.fl_str_mv |
Aguiar,Ana Paula Costa,Ana Rosa Correr,Américo Bortolazzo Vedovello,Silvia Amélia Vedovello Filho,Mário Crepaldi,Marcus Vinicius Valdrighi,Heloísa Cristina Correr-Sobrinho,Lourenço |
dc.subject.por.fl_str_mv |
ceramic dental materials hydrofluoric acid thermal cycling orthodontic |
topic |
ceramic dental materials hydrofluoric acid thermal cycling orthodontic |
description |
Abstract This study to evaluate the effects of different hydrofluoric acid (HF) concentrations and thermal cycling on the shear bond strength (SBS) of brackets to ceramic. Cylinders of ceramic were divided into 10 groups (n=15), according to HF concentrations: 1-1%;2-2.5%;3-5%;4-7.5%;5-10% (storage 24 h); 6-1%;7-2.5%;8-5%;9-7.5%; and, 10-10% (thermal cycling). All cylinders were etched for 60s and received one layer of silane. Metallic brackets were bonded to the cylinders using Transbond-XT, light activated for 40 s, using a LED (Radii Plus) and stored in deionized water at 37o C for 24h. The groups 6 to 10 were submitted to thermal cycling (7,000 cycles - 5o/55oC). SBS was performed in an Instron at crosshead speed of 1.0 mm/min. Data were submitted to two-way ANOVA and Tukey’s post-hoc test (α=0.05). The Adhesive Remaining Index (ARI) was evaluated at 40x magnification. The different HF acid concentrations influenced on the SBS of the brackets to ceramic (p<0.05). The thermal cycling decreased the SBS of the brackets to ceramic for all acid concentrations (p<0.05). The ARI showed a predominance of scores 0 for all groups, with an increase in scores 1, 2 and 3 for the group storage for 24 h. In conclusion, the different HF acid concentrations 5.0%, 7.5% and 10% influenced on the SBS of brackets to ceramic. The thermal cycling decreased significantly the SBS of brackets to ceramic. |
publishDate |
2019 |
dc.date.none.fl_str_mv |
2019-11-01 |
dc.type.driver.fl_str_mv |
info:eu-repo/semantics/article |
dc.type.status.fl_str_mv |
info:eu-repo/semantics/publishedVersion |
format |
article |
status_str |
publishedVersion |
dc.identifier.uri.fl_str_mv |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0103-64402019000600587 |
url |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0103-64402019000600587 |
dc.language.iso.fl_str_mv |
eng |
language |
eng |
dc.relation.none.fl_str_mv |
10.1590/0103-6440201902989 |
dc.rights.driver.fl_str_mv |
info:eu-repo/semantics/openAccess |
eu_rights_str_mv |
openAccess |
dc.format.none.fl_str_mv |
text/html |
dc.publisher.none.fl_str_mv |
Fundação Odontológica de Ribeirão Preto |
publisher.none.fl_str_mv |
Fundação Odontológica de Ribeirão Preto |
dc.source.none.fl_str_mv |
Brazilian Dental Journal v.30 n.6 2019 reponame:Brazilian Dental Journal instname:Fundação Odontológica de Ribeirão Preto (FUNORP) instacron:FUNORP |
instname_str |
Fundação Odontológica de Ribeirão Preto (FUNORP) |
instacron_str |
FUNORP |
institution |
FUNORP |
reponame_str |
Brazilian Dental Journal |
collection |
Brazilian Dental Journal |
repository.name.fl_str_mv |
Brazilian Dental Journal - Fundação Odontológica de Ribeirão Preto (FUNORP) |
repository.mail.fl_str_mv |
bdj@forp.usp.br||sergio@fosjc.unesp.br |
_version_ |
1754204095751651328 |