Experimental analysis of reinforced concrete columns strengthened with self-compacting concrete and connectors

Detalhes bibliográficos
Autor(a) principal: Nascimento,P. P.
Data de Publicação: 2012
Outros Autores: Gomes,R. B., Borges,L. L. J., David,D. L.
Tipo de documento: Artigo
Idioma: eng
Título da fonte: Revista IBRACON de Estruturas e Materiais
Texto Completo: http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1983-41952012000300004
Resumo: There are many problems involving cases of destruction of buildings and other structures. The columns can deteriorate for several reasons such as the evolution and changing habits of the loads. The experimental phase of this work was based on a test involving nine reinforced concrete columns under combined bending and axial compression, at an initial eccentricity of 60 mm. Two columns were used as reference, one having the original dimensions of the column and the other, monolithic, had been cast along the thickness of the strengthened piece. The remaining columns received a 35 mm thick layer of self-compacting concrete on their compressed face. For the preparation of the interface between the two materials, this surface was scarified and furrowed and connectors were inserted onto the columns' shear reinforcement in various positions and amounts.As connectors, 5 mm diameter steel bars were used (the same as for stirrups), bent in the shape of a "C" with 25 mm coatings. >As a conclusion, not only the quantity, but mainly, the location of the connectors used in the link between substrate and reinforcement is crucial to increase strength and to change failure mode.
id IBRACON-1_2e0342c0c55225f198ae356a87039538
oai_identifier_str oai:scielo:S1983-41952012000300004
network_acronym_str IBRACON-1
network_name_str Revista IBRACON de Estruturas e Materiais
repository_id_str
spelling Experimental analysis of reinforced concrete columns strengthened with self-compacting concrete and connectorssreinforced concretecolumnsself-compacting concreteconnectorseccentric loadThere are many problems involving cases of destruction of buildings and other structures. The columns can deteriorate for several reasons such as the evolution and changing habits of the loads. The experimental phase of this work was based on a test involving nine reinforced concrete columns under combined bending and axial compression, at an initial eccentricity of 60 mm. Two columns were used as reference, one having the original dimensions of the column and the other, monolithic, had been cast along the thickness of the strengthened piece. The remaining columns received a 35 mm thick layer of self-compacting concrete on their compressed face. For the preparation of the interface between the two materials, this surface was scarified and furrowed and connectors were inserted onto the columns' shear reinforcement in various positions and amounts.As connectors, 5 mm diameter steel bars were used (the same as for stirrups), bent in the shape of a "C" with 25 mm coatings. >As a conclusion, not only the quantity, but mainly, the location of the connectors used in the link between substrate and reinforcement is crucial to increase strength and to change failure mode.IBRACON - Instituto Brasileiro do Concreto2012-06-01info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersiontext/htmlhttp://old.scielo.br/scielo.php?script=sci_arttext&pid=S1983-41952012000300004Revista IBRACON de Estruturas e Materiais v.5 n.3 2012reponame:Revista IBRACON de Estruturas e Materiaisinstname:Instituto Brasileiro do Concreto (IBRACON)instacron:IBRACON10.1590/S1983-41952012000300004info:eu-repo/semantics/openAccessNascimento,P. P.Gomes,R. B.Borges,L. L. J.David,D. L.eng2012-09-20T00:00:00Zoai:scielo:S1983-41952012000300004Revistahttp://www.revistas.ibracon.org.br/index.php/riemhttps://old.scielo.br/oai/scielo-oai.phpeditores.riem@gmail.com||arlene@ibracon.org.br1983-41951983-4195opendoar:2012-09-20T00:00Revista IBRACON de Estruturas e Materiais - Instituto Brasileiro do Concreto (IBRACON)false
dc.title.none.fl_str_mv Experimental analysis of reinforced concrete columns strengthened with self-compacting concrete and connectors
title Experimental analysis of reinforced concrete columns strengthened with self-compacting concrete and connectors
spellingShingle Experimental analysis of reinforced concrete columns strengthened with self-compacting concrete and connectors
Nascimento,P. P.
sreinforced concrete
columns
self-compacting concrete
connectors
eccentric load
title_short Experimental analysis of reinforced concrete columns strengthened with self-compacting concrete and connectors
title_full Experimental analysis of reinforced concrete columns strengthened with self-compacting concrete and connectors
title_fullStr Experimental analysis of reinforced concrete columns strengthened with self-compacting concrete and connectors
title_full_unstemmed Experimental analysis of reinforced concrete columns strengthened with self-compacting concrete and connectors
title_sort Experimental analysis of reinforced concrete columns strengthened with self-compacting concrete and connectors
author Nascimento,P. P.
author_facet Nascimento,P. P.
Gomes,R. B.
Borges,L. L. J.
David,D. L.
author_role author
author2 Gomes,R. B.
Borges,L. L. J.
David,D. L.
author2_role author
author
author
dc.contributor.author.fl_str_mv Nascimento,P. P.
Gomes,R. B.
Borges,L. L. J.
David,D. L.
dc.subject.por.fl_str_mv sreinforced concrete
columns
self-compacting concrete
connectors
eccentric load
topic sreinforced concrete
columns
self-compacting concrete
connectors
eccentric load
description There are many problems involving cases of destruction of buildings and other structures. The columns can deteriorate for several reasons such as the evolution and changing habits of the loads. The experimental phase of this work was based on a test involving nine reinforced concrete columns under combined bending and axial compression, at an initial eccentricity of 60 mm. Two columns were used as reference, one having the original dimensions of the column and the other, monolithic, had been cast along the thickness of the strengthened piece. The remaining columns received a 35 mm thick layer of self-compacting concrete on their compressed face. For the preparation of the interface between the two materials, this surface was scarified and furrowed and connectors were inserted onto the columns' shear reinforcement in various positions and amounts.As connectors, 5 mm diameter steel bars were used (the same as for stirrups), bent in the shape of a "C" with 25 mm coatings. >As a conclusion, not only the quantity, but mainly, the location of the connectors used in the link between substrate and reinforcement is crucial to increase strength and to change failure mode.
publishDate 2012
dc.date.none.fl_str_mv 2012-06-01
dc.type.driver.fl_str_mv info:eu-repo/semantics/article
dc.type.status.fl_str_mv info:eu-repo/semantics/publishedVersion
format article
status_str publishedVersion
dc.identifier.uri.fl_str_mv http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1983-41952012000300004
url http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1983-41952012000300004
dc.language.iso.fl_str_mv eng
language eng
dc.relation.none.fl_str_mv 10.1590/S1983-41952012000300004
dc.rights.driver.fl_str_mv info:eu-repo/semantics/openAccess
eu_rights_str_mv openAccess
dc.format.none.fl_str_mv text/html
dc.publisher.none.fl_str_mv IBRACON - Instituto Brasileiro do Concreto
publisher.none.fl_str_mv IBRACON - Instituto Brasileiro do Concreto
dc.source.none.fl_str_mv Revista IBRACON de Estruturas e Materiais v.5 n.3 2012
reponame:Revista IBRACON de Estruturas e Materiais
instname:Instituto Brasileiro do Concreto (IBRACON)
instacron:IBRACON
instname_str Instituto Brasileiro do Concreto (IBRACON)
instacron_str IBRACON
institution IBRACON
reponame_str Revista IBRACON de Estruturas e Materiais
collection Revista IBRACON de Estruturas e Materiais
repository.name.fl_str_mv Revista IBRACON de Estruturas e Materiais - Instituto Brasileiro do Concreto (IBRACON)
repository.mail.fl_str_mv editores.riem@gmail.com||arlene@ibracon.org.br
_version_ 1754193604357652480