Resumo: | Fe-clay catalysts have been prepared and tested for Orange II oxidation with H2O2 in aqueous solution. The reaction is carried out in a batch reactor, using different hydrogen peroxide concentrations, and in a wide range of temperature and pH values. Twelve samples were prepared, with three different iron loads (7.5, 13.0 and 17.0 %, w/w), and using four iron salts as precursors, namely Fe(II) acetate, Fe(II) oxalate, Fe(II) acetylacetonate and Fe(III) acetylacetonate. The samples were characterized using X-ray diffraction, thermal analysis, infrared spectroscopy and adsorption of nitrogen at 77K. The catalytic results show that these solids present good catalytic properties for the degradation and mineralization of Orange II solutions, allowing to reach, in the best conditions and after 4h of oxidation, 99% of dye degradation with 91% of TOC (Total Organic Carbon) reduction (at 70ºC), using only ca. 90 mg of clay catalyst per litre of solution. Nevertheless, 96% of dye removal with 82% of mineralization were also reached at 30ºC. Besides, the amount of iron released into the final solution is lower than 1 ppm, in the worst of the cases, and 0.09 ppm in the best case. |
id |
RCAP_0e763b9055cfcf79d62b5f2c5aa79b30 |
---|---|
oai_identifier_str |
oai:repositorio-aberto.up.pt:10216/69418 |
network_acronym_str |
RCAP |
network_name_str |
Repositório Científico de Acesso Aberto de Portugal (Repositórios Cientìficos) |
repository_id_str |
7160 |
spelling |
Fenton-like oxidation of Orange II solutions using heterogeneous catalysts based on saponite clayEngenharia químicaChemical engineeringFe-clay catalysts have been prepared and tested for Orange II oxidation with H2O2 in aqueous solution. The reaction is carried out in a batch reactor, using different hydrogen peroxide concentrations, and in a wide range of temperature and pH values. Twelve samples were prepared, with three different iron loads (7.5, 13.0 and 17.0 %, w/w), and using four iron salts as precursors, namely Fe(II) acetate, Fe(II) oxalate, Fe(II) acetylacetonate and Fe(III) acetylacetonate. The samples were characterized using X-ray diffraction, thermal analysis, infrared spectroscopy and adsorption of nitrogen at 77K. The catalytic results show that these solids present good catalytic properties for the degradation and mineralization of Orange II solutions, allowing to reach, in the best conditions and after 4h of oxidation, 99% of dye degradation with 91% of TOC (Total Organic Carbon) reduction (at 70ºC), using only ca. 90 mg of clay catalyst per litre of solution. Nevertheless, 96% of dye removal with 82% of mineralization were also reached at 30ºC. Besides, the amount of iron released into the final solution is lower than 1 ppm, in the worst of the cases, and 0.09 ppm in the best case.20062006-01-01T00:00:00Zinfo:eu-repo/semantics/publishedVersioninfo:eu-repo/semantics/bookapplication/pdfhttps://hdl.handle.net/10216/69418engJ. Herney RamirezCarlos A. CostaLuís M. MadeiraG. MataMiguel A. VicenteM. L. Rojas CervantesR. M. Martín Arandainfo:eu-repo/semantics/openAccessreponame:Repositório Científico de Acesso Aberto de Portugal (Repositórios Cientìficos)instname:Agência para a Sociedade do Conhecimento (UMIC) - FCT - Sociedade da Informaçãoinstacron:RCAAP2023-11-29T14:15:12Zoai:repositorio-aberto.up.pt:10216/69418Portal AgregadorONGhttps://www.rcaap.pt/oai/openaireopendoar:71602024-03-19T23:57:44.788507Repositório Científico de Acesso Aberto de Portugal (Repositórios Cientìficos) - Agência para a Sociedade do Conhecimento (UMIC) - FCT - Sociedade da Informaçãofalse |
dc.title.none.fl_str_mv |
Fenton-like oxidation of Orange II solutions using heterogeneous catalysts based on saponite clay |
title |
Fenton-like oxidation of Orange II solutions using heterogeneous catalysts based on saponite clay |
spellingShingle |
Fenton-like oxidation of Orange II solutions using heterogeneous catalysts based on saponite clay J. Herney Ramirez Engenharia química Chemical engineering |
title_short |
Fenton-like oxidation of Orange II solutions using heterogeneous catalysts based on saponite clay |
title_full |
Fenton-like oxidation of Orange II solutions using heterogeneous catalysts based on saponite clay |
title_fullStr |
Fenton-like oxidation of Orange II solutions using heterogeneous catalysts based on saponite clay |
title_full_unstemmed |
Fenton-like oxidation of Orange II solutions using heterogeneous catalysts based on saponite clay |
title_sort |
Fenton-like oxidation of Orange II solutions using heterogeneous catalysts based on saponite clay |
author |
J. Herney Ramirez |
author_facet |
J. Herney Ramirez Carlos A. Costa Luís M. Madeira G. Mata Miguel A. Vicente M. L. Rojas Cervantes R. M. Martín Aranda |
author_role |
author |
author2 |
Carlos A. Costa Luís M. Madeira G. Mata Miguel A. Vicente M. L. Rojas Cervantes R. M. Martín Aranda |
author2_role |
author author author author author author |
dc.contributor.author.fl_str_mv |
J. Herney Ramirez Carlos A. Costa Luís M. Madeira G. Mata Miguel A. Vicente M. L. Rojas Cervantes R. M. Martín Aranda |
dc.subject.por.fl_str_mv |
Engenharia química Chemical engineering |
topic |
Engenharia química Chemical engineering |
description |
Fe-clay catalysts have been prepared and tested for Orange II oxidation with H2O2 in aqueous solution. The reaction is carried out in a batch reactor, using different hydrogen peroxide concentrations, and in a wide range of temperature and pH values. Twelve samples were prepared, with three different iron loads (7.5, 13.0 and 17.0 %, w/w), and using four iron salts as precursors, namely Fe(II) acetate, Fe(II) oxalate, Fe(II) acetylacetonate and Fe(III) acetylacetonate. The samples were characterized using X-ray diffraction, thermal analysis, infrared spectroscopy and adsorption of nitrogen at 77K. The catalytic results show that these solids present good catalytic properties for the degradation and mineralization of Orange II solutions, allowing to reach, in the best conditions and after 4h of oxidation, 99% of dye degradation with 91% of TOC (Total Organic Carbon) reduction (at 70ºC), using only ca. 90 mg of clay catalyst per litre of solution. Nevertheless, 96% of dye removal with 82% of mineralization were also reached at 30ºC. Besides, the amount of iron released into the final solution is lower than 1 ppm, in the worst of the cases, and 0.09 ppm in the best case. |
publishDate |
2006 |
dc.date.none.fl_str_mv |
2006 2006-01-01T00:00:00Z |
dc.type.status.fl_str_mv |
info:eu-repo/semantics/publishedVersion |
dc.type.driver.fl_str_mv |
info:eu-repo/semantics/book |
format |
book |
status_str |
publishedVersion |
dc.identifier.uri.fl_str_mv |
https://hdl.handle.net/10216/69418 |
url |
https://hdl.handle.net/10216/69418 |
dc.language.iso.fl_str_mv |
eng |
language |
eng |
dc.rights.driver.fl_str_mv |
info:eu-repo/semantics/openAccess |
eu_rights_str_mv |
openAccess |
dc.format.none.fl_str_mv |
application/pdf |
dc.source.none.fl_str_mv |
reponame:Repositório Científico de Acesso Aberto de Portugal (Repositórios Cientìficos) instname:Agência para a Sociedade do Conhecimento (UMIC) - FCT - Sociedade da Informação instacron:RCAAP |
instname_str |
Agência para a Sociedade do Conhecimento (UMIC) - FCT - Sociedade da Informação |
instacron_str |
RCAAP |
institution |
RCAAP |
reponame_str |
Repositório Científico de Acesso Aberto de Portugal (Repositórios Cientìficos) |
collection |
Repositório Científico de Acesso Aberto de Portugal (Repositórios Cientìficos) |
repository.name.fl_str_mv |
Repositório Científico de Acesso Aberto de Portugal (Repositórios Cientìficos) - Agência para a Sociedade do Conhecimento (UMIC) - FCT - Sociedade da Informação |
repository.mail.fl_str_mv |
|
_version_ |
1799135899279163392 |