Atmospheric corrosion of Nylon 6,6 in Mauritius
Autor(a) principal: | |
---|---|
Data de Publicação: | 2016 |
Outros Autores: | |
Tipo de documento: | Artigo |
Idioma: | eng |
Título da fonte: | Matéria (Rio de Janeiro. Online) |
Texto Completo: | http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1517-70762016000400841 |
Resumo: | ABSTRACT Plastics are being more and more commonly used for outdoor applications in Mauritius. In this context, the atmospheric corrosion degradation behaviour of nylon 6,6 was observed in the Mauritian atmosphere, having a corrosivity category of C3, according to ISO 9223. The crack width, depth and extent of the cracks formed on the surface were investigated using micrometry and image analysis. The changes in the chemical composition of the nylon 6,6 were investigated using the Fourier Transform Infrared spectroscopy technique. It was observed that the nylon 6,6 surface showed a progressive discolouration and a sudden increase in the size of the cracks after around 2 years of exposure. The degree of crack formation in terms of crack width, the depth of degradation and the microhardness of the surface were evaluated and all showed significant degradation only after about 2 years of exposure. Degradation has penetrated the test material within 750 µm from the surface in 4.5 years of exposure. Using the FTIR technique, evidence of chain scission occurring among the polymer chains was observed. |
id |
RLAM-1_4ddc7c2240909109125a62a47764a438 |
---|---|
oai_identifier_str |
oai:scielo:S1517-70762016000400841 |
network_acronym_str |
RLAM-1 |
network_name_str |
Matéria (Rio de Janeiro. Online) |
repository_id_str |
|
spelling |
Atmospheric corrosion of Nylon 6,6 in Mauritiusnylonatmospheric corrosionweatheringcracksFTIRABSTRACT Plastics are being more and more commonly used for outdoor applications in Mauritius. In this context, the atmospheric corrosion degradation behaviour of nylon 6,6 was observed in the Mauritian atmosphere, having a corrosivity category of C3, according to ISO 9223. The crack width, depth and extent of the cracks formed on the surface were investigated using micrometry and image analysis. The changes in the chemical composition of the nylon 6,6 were investigated using the Fourier Transform Infrared spectroscopy technique. It was observed that the nylon 6,6 surface showed a progressive discolouration and a sudden increase in the size of the cracks after around 2 years of exposure. The degree of crack formation in terms of crack width, the depth of degradation and the microhardness of the surface were evaluated and all showed significant degradation only after about 2 years of exposure. Degradation has penetrated the test material within 750 µm from the surface in 4.5 years of exposure. Using the FTIR technique, evidence of chain scission occurring among the polymer chains was observed.Laboratório de Hidrogênio, Coppe - Universidade Federal do Rio de Janeiroem cooperação com a Associação Brasileira do Hidrogênio, ABH22016-12-01info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersiontext/htmlhttp://old.scielo.br/scielo.php?script=sci_arttext&pid=S1517-70762016000400841Matéria (Rio de Janeiro) v.21 n.4 2016reponame:Matéria (Rio de Janeiro. Online)instname:Matéria (Rio de Janeiro. Online)instacron:RLAM10.1590/s1517-707620160004.0080info:eu-repo/semantics/openAccessTew,David HonSurnam,Baboo Yashwansingh Ranveersingheng2016-12-19T00:00:00Zoai:scielo:S1517-70762016000400841Revistahttp://www.materia.coppe.ufrj.br/https://old.scielo.br/oai/scielo-oai.php||materia@labh2.coppe.ufrj.br1517-70761517-7076opendoar:2016-12-19T00:00Matéria (Rio de Janeiro. Online) - Matéria (Rio de Janeiro. Online)false |
dc.title.none.fl_str_mv |
Atmospheric corrosion of Nylon 6,6 in Mauritius |
title |
Atmospheric corrosion of Nylon 6,6 in Mauritius |
spellingShingle |
Atmospheric corrosion of Nylon 6,6 in Mauritius Tew,David Hon nylon atmospheric corrosion weathering cracks FTIR |
title_short |
Atmospheric corrosion of Nylon 6,6 in Mauritius |
title_full |
Atmospheric corrosion of Nylon 6,6 in Mauritius |
title_fullStr |
Atmospheric corrosion of Nylon 6,6 in Mauritius |
title_full_unstemmed |
Atmospheric corrosion of Nylon 6,6 in Mauritius |
title_sort |
Atmospheric corrosion of Nylon 6,6 in Mauritius |
author |
Tew,David Hon |
author_facet |
Tew,David Hon Surnam,Baboo Yashwansingh Ranveersingh |
author_role |
author |
author2 |
Surnam,Baboo Yashwansingh Ranveersingh |
author2_role |
author |
dc.contributor.author.fl_str_mv |
Tew,David Hon Surnam,Baboo Yashwansingh Ranveersingh |
dc.subject.por.fl_str_mv |
nylon atmospheric corrosion weathering cracks FTIR |
topic |
nylon atmospheric corrosion weathering cracks FTIR |
description |
ABSTRACT Plastics are being more and more commonly used for outdoor applications in Mauritius. In this context, the atmospheric corrosion degradation behaviour of nylon 6,6 was observed in the Mauritian atmosphere, having a corrosivity category of C3, according to ISO 9223. The crack width, depth and extent of the cracks formed on the surface were investigated using micrometry and image analysis. The changes in the chemical composition of the nylon 6,6 were investigated using the Fourier Transform Infrared spectroscopy technique. It was observed that the nylon 6,6 surface showed a progressive discolouration and a sudden increase in the size of the cracks after around 2 years of exposure. The degree of crack formation in terms of crack width, the depth of degradation and the microhardness of the surface were evaluated and all showed significant degradation only after about 2 years of exposure. Degradation has penetrated the test material within 750 µm from the surface in 4.5 years of exposure. Using the FTIR technique, evidence of chain scission occurring among the polymer chains was observed. |
publishDate |
2016 |
dc.date.none.fl_str_mv |
2016-12-01 |
dc.type.driver.fl_str_mv |
info:eu-repo/semantics/article |
dc.type.status.fl_str_mv |
info:eu-repo/semantics/publishedVersion |
format |
article |
status_str |
publishedVersion |
dc.identifier.uri.fl_str_mv |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1517-70762016000400841 |
url |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1517-70762016000400841 |
dc.language.iso.fl_str_mv |
eng |
language |
eng |
dc.relation.none.fl_str_mv |
10.1590/s1517-707620160004.0080 |
dc.rights.driver.fl_str_mv |
info:eu-repo/semantics/openAccess |
eu_rights_str_mv |
openAccess |
dc.format.none.fl_str_mv |
text/html |
dc.publisher.none.fl_str_mv |
Laboratório de Hidrogênio, Coppe - Universidade Federal do Rio de Janeiro em cooperação com a Associação Brasileira do Hidrogênio, ABH2 |
publisher.none.fl_str_mv |
Laboratório de Hidrogênio, Coppe - Universidade Federal do Rio de Janeiro em cooperação com a Associação Brasileira do Hidrogênio, ABH2 |
dc.source.none.fl_str_mv |
Matéria (Rio de Janeiro) v.21 n.4 2016 reponame:Matéria (Rio de Janeiro. Online) instname:Matéria (Rio de Janeiro. Online) instacron:RLAM |
instname_str |
Matéria (Rio de Janeiro. Online) |
instacron_str |
RLAM |
institution |
RLAM |
reponame_str |
Matéria (Rio de Janeiro. Online) |
collection |
Matéria (Rio de Janeiro. Online) |
repository.name.fl_str_mv |
Matéria (Rio de Janeiro. Online) - Matéria (Rio de Janeiro. Online) |
repository.mail.fl_str_mv |
||materia@labh2.coppe.ufrj.br |
_version_ |
1752126689324826624 |