Morphological study of Sr2CeO4 blue phosphor with fine particles
Autor(a) principal: | |
---|---|
Data de Publicação: | 2004 |
Outros Autores: | , |
Tipo de documento: | Artigo |
Idioma: | eng |
Título da fonte: | Química Nova (Online) |
Texto Completo: | http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422004000500005 |
Resumo: | Morphological and spectroscopic studies of Sr2CeO4 blue phosphor in the form of fine particles prepared from a powdered multi-component precursor, via a combustion method, are reported. Samples were also prepared through a solid-state reaction and from a polymeric precursor for comparison. Citric acid or glycine as fuels in the combustion method lead to a mixture which is heated at 950 ºC for 4 h, resulting in spheroidal particles with a diameter between 250-550 nm. Samples from the polymeric precursor result in spheroidal particles (350-550 nm) and from the solid-state reaction in irregular particles (~ 5 mum). Therefore, the combustion method is adequate for preparation of Sr2CeO4 in the form of spherical fine particles. |
id |
SBQ-3_064aeb97264141be670f6db49e66cb57 |
---|---|
oai_identifier_str |
oai:scielo:S0100-40422004000500005 |
network_acronym_str |
SBQ-3 |
network_name_str |
Química Nova (Online) |
repository_id_str |
|
spelling |
Morphological study of Sr2CeO4 blue phosphor with fine particlesblue phosphorcombustion methodfine spheroidal particlesMorphological and spectroscopic studies of Sr2CeO4 blue phosphor in the form of fine particles prepared from a powdered multi-component precursor, via a combustion method, are reported. Samples were also prepared through a solid-state reaction and from a polymeric precursor for comparison. Citric acid or glycine as fuels in the combustion method lead to a mixture which is heated at 950 ºC for 4 h, resulting in spheroidal particles with a diameter between 250-550 nm. Samples from the polymeric precursor result in spheroidal particles (350-550 nm) and from the solid-state reaction in irregular particles (~ 5 mum). Therefore, the combustion method is adequate for preparation of Sr2CeO4 in the form of spherical fine particles.Sociedade Brasileira de Química2004-10-01info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersiontext/htmlhttp://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422004000500005Química Nova v.27 n.5 2004reponame:Química Nova (Online)instname:Sociedade Brasileira de Química (SBQ)instacron:SBQ10.1590/S0100-40422004000500005info:eu-repo/semantics/openAccessGomes,JanaínaPires,Ana MariaSerra,Osvaldo Antonioeng2004-09-17T00:00:00Zoai:scielo:S0100-40422004000500005Revistahttps://www.scielo.br/j/qn/ONGhttps://old.scielo.br/oai/scielo-oai.phpquimicanova@sbq.org.br1678-70640100-4042opendoar:2004-09-17T00:00Química Nova (Online) - Sociedade Brasileira de Química (SBQ)false |
dc.title.none.fl_str_mv |
Morphological study of Sr2CeO4 blue phosphor with fine particles |
title |
Morphological study of Sr2CeO4 blue phosphor with fine particles |
spellingShingle |
Morphological study of Sr2CeO4 blue phosphor with fine particles Gomes,Janaína blue phosphor combustion method fine spheroidal particles |
title_short |
Morphological study of Sr2CeO4 blue phosphor with fine particles |
title_full |
Morphological study of Sr2CeO4 blue phosphor with fine particles |
title_fullStr |
Morphological study of Sr2CeO4 blue phosphor with fine particles |
title_full_unstemmed |
Morphological study of Sr2CeO4 blue phosphor with fine particles |
title_sort |
Morphological study of Sr2CeO4 blue phosphor with fine particles |
author |
Gomes,Janaína |
author_facet |
Gomes,Janaína Pires,Ana Maria Serra,Osvaldo Antonio |
author_role |
author |
author2 |
Pires,Ana Maria Serra,Osvaldo Antonio |
author2_role |
author author |
dc.contributor.author.fl_str_mv |
Gomes,Janaína Pires,Ana Maria Serra,Osvaldo Antonio |
dc.subject.por.fl_str_mv |
blue phosphor combustion method fine spheroidal particles |
topic |
blue phosphor combustion method fine spheroidal particles |
description |
Morphological and spectroscopic studies of Sr2CeO4 blue phosphor in the form of fine particles prepared from a powdered multi-component precursor, via a combustion method, are reported. Samples were also prepared through a solid-state reaction and from a polymeric precursor for comparison. Citric acid or glycine as fuels in the combustion method lead to a mixture which is heated at 950 ºC for 4 h, resulting in spheroidal particles with a diameter between 250-550 nm. Samples from the polymeric precursor result in spheroidal particles (350-550 nm) and from the solid-state reaction in irregular particles (~ 5 mum). Therefore, the combustion method is adequate for preparation of Sr2CeO4 in the form of spherical fine particles. |
publishDate |
2004 |
dc.date.none.fl_str_mv |
2004-10-01 |
dc.type.driver.fl_str_mv |
info:eu-repo/semantics/article |
dc.type.status.fl_str_mv |
info:eu-repo/semantics/publishedVersion |
format |
article |
status_str |
publishedVersion |
dc.identifier.uri.fl_str_mv |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422004000500005 |
url |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422004000500005 |
dc.language.iso.fl_str_mv |
eng |
language |
eng |
dc.relation.none.fl_str_mv |
10.1590/S0100-40422004000500005 |
dc.rights.driver.fl_str_mv |
info:eu-repo/semantics/openAccess |
eu_rights_str_mv |
openAccess |
dc.format.none.fl_str_mv |
text/html |
dc.publisher.none.fl_str_mv |
Sociedade Brasileira de Química |
publisher.none.fl_str_mv |
Sociedade Brasileira de Química |
dc.source.none.fl_str_mv |
Química Nova v.27 n.5 2004 reponame:Química Nova (Online) instname:Sociedade Brasileira de Química (SBQ) instacron:SBQ |
instname_str |
Sociedade Brasileira de Química (SBQ) |
instacron_str |
SBQ |
institution |
SBQ |
reponame_str |
Química Nova (Online) |
collection |
Química Nova (Online) |
repository.name.fl_str_mv |
Química Nova (Online) - Sociedade Brasileira de Química (SBQ) |
repository.mail.fl_str_mv |
quimicanova@sbq.org.br |
_version_ |
1750318103890231296 |