EFEITOS DA TEMPERATURA NOS ESPECTROS RAMAN DOS POLÍMEROS CONDUTORES PEDOT E MEH-PPV
Autor(a) principal: | |
---|---|
Data de Publicação: | 2019 |
Outros Autores: | , |
Tipo de documento: | Artigo |
Idioma: | por |
Título da fonte: | Química Nova (Online) |
Texto Completo: | http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422019004901098 |
Resumo: | The present work shows the temperature dependence of the Raman spectra of two conjugated polymers: poly[2-methoxy-5-(2-ethylhexyloxy)-1,4-phenylenevinylene] (MEH-PPV) and poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonate) (PEDOT:PSS). In situ resonance Raman spectra of PEDOT from 77 to 423 K at 633 nm and of MEH-PPV from 77 to 473 K at 785 nm suggest that, for both polymers, as the temperature increases there is a decrease in the chain conjugation length. Raman bands of PEDOT assigned to the νsim Cα-Cβ are the most sensitive to temperature while bands due to oxyethylene rings do not show significant shifts in this temperature range. Raman and FT-IR spectra of MEH-PPV recorded above the thermal decomposition temperature provide some insights about the thermal degradation. |
id |
SBQ-3_328e1903465fbf5cfb8023f0d223d466 |
---|---|
oai_identifier_str |
oai:scielo:S0100-40422019004901098 |
network_acronym_str |
SBQ-3 |
network_name_str |
Química Nova (Online) |
repository_id_str |
|
spelling |
EFEITOS DA TEMPERATURA NOS ESPECTROS RAMAN DOS POLÍMEROS CONDUTORES PEDOT E MEH-PPVRaman spectroscopyMEH-PPVPEDOTin situ Raman, conducting polymerThe present work shows the temperature dependence of the Raman spectra of two conjugated polymers: poly[2-methoxy-5-(2-ethylhexyloxy)-1,4-phenylenevinylene] (MEH-PPV) and poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonate) (PEDOT:PSS). In situ resonance Raman spectra of PEDOT from 77 to 423 K at 633 nm and of MEH-PPV from 77 to 473 K at 785 nm suggest that, for both polymers, as the temperature increases there is a decrease in the chain conjugation length. Raman bands of PEDOT assigned to the νsim Cα-Cβ are the most sensitive to temperature while bands due to oxyethylene rings do not show significant shifts in this temperature range. Raman and FT-IR spectra of MEH-PPV recorded above the thermal decomposition temperature provide some insights about the thermal degradation.Sociedade Brasileira de Química2019-09-01info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersiontext/htmlhttp://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422019004901098Química Nova v.42 n.9 2019reponame:Química Nova (Online)instname:Sociedade Brasileira de Química (SBQ)instacron:SBQ10.21577/0100-4042.20170425info:eu-repo/semantics/openAccessBarra,Alvaro C. C.Amaral,Thaeny C.Izumi,Celly M. S.por2019-12-09T00:00:00Zoai:scielo:S0100-40422019004901098Revistahttps://www.scielo.br/j/qn/ONGhttps://old.scielo.br/oai/scielo-oai.phpquimicanova@sbq.org.br1678-70640100-4042opendoar:2019-12-09T00:00Química Nova (Online) - Sociedade Brasileira de Química (SBQ)false |
dc.title.none.fl_str_mv |
EFEITOS DA TEMPERATURA NOS ESPECTROS RAMAN DOS POLÍMEROS CONDUTORES PEDOT E MEH-PPV |
title |
EFEITOS DA TEMPERATURA NOS ESPECTROS RAMAN DOS POLÍMEROS CONDUTORES PEDOT E MEH-PPV |
spellingShingle |
EFEITOS DA TEMPERATURA NOS ESPECTROS RAMAN DOS POLÍMEROS CONDUTORES PEDOT E MEH-PPV Barra,Alvaro C. C. Raman spectroscopy MEH-PPV PEDOT in situ Raman, conducting polymer |
title_short |
EFEITOS DA TEMPERATURA NOS ESPECTROS RAMAN DOS POLÍMEROS CONDUTORES PEDOT E MEH-PPV |
title_full |
EFEITOS DA TEMPERATURA NOS ESPECTROS RAMAN DOS POLÍMEROS CONDUTORES PEDOT E MEH-PPV |
title_fullStr |
EFEITOS DA TEMPERATURA NOS ESPECTROS RAMAN DOS POLÍMEROS CONDUTORES PEDOT E MEH-PPV |
title_full_unstemmed |
EFEITOS DA TEMPERATURA NOS ESPECTROS RAMAN DOS POLÍMEROS CONDUTORES PEDOT E MEH-PPV |
title_sort |
EFEITOS DA TEMPERATURA NOS ESPECTROS RAMAN DOS POLÍMEROS CONDUTORES PEDOT E MEH-PPV |
author |
Barra,Alvaro C. C. |
author_facet |
Barra,Alvaro C. C. Amaral,Thaeny C. Izumi,Celly M. S. |
author_role |
author |
author2 |
Amaral,Thaeny C. Izumi,Celly M. S. |
author2_role |
author author |
dc.contributor.author.fl_str_mv |
Barra,Alvaro C. C. Amaral,Thaeny C. Izumi,Celly M. S. |
dc.subject.por.fl_str_mv |
Raman spectroscopy MEH-PPV PEDOT in situ Raman, conducting polymer |
topic |
Raman spectroscopy MEH-PPV PEDOT in situ Raman, conducting polymer |
description |
The present work shows the temperature dependence of the Raman spectra of two conjugated polymers: poly[2-methoxy-5-(2-ethylhexyloxy)-1,4-phenylenevinylene] (MEH-PPV) and poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonate) (PEDOT:PSS). In situ resonance Raman spectra of PEDOT from 77 to 423 K at 633 nm and of MEH-PPV from 77 to 473 K at 785 nm suggest that, for both polymers, as the temperature increases there is a decrease in the chain conjugation length. Raman bands of PEDOT assigned to the νsim Cα-Cβ are the most sensitive to temperature while bands due to oxyethylene rings do not show significant shifts in this temperature range. Raman and FT-IR spectra of MEH-PPV recorded above the thermal decomposition temperature provide some insights about the thermal degradation. |
publishDate |
2019 |
dc.date.none.fl_str_mv |
2019-09-01 |
dc.type.driver.fl_str_mv |
info:eu-repo/semantics/article |
dc.type.status.fl_str_mv |
info:eu-repo/semantics/publishedVersion |
format |
article |
status_str |
publishedVersion |
dc.identifier.uri.fl_str_mv |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422019004901098 |
url |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422019004901098 |
dc.language.iso.fl_str_mv |
por |
language |
por |
dc.relation.none.fl_str_mv |
10.21577/0100-4042.20170425 |
dc.rights.driver.fl_str_mv |
info:eu-repo/semantics/openAccess |
eu_rights_str_mv |
openAccess |
dc.format.none.fl_str_mv |
text/html |
dc.publisher.none.fl_str_mv |
Sociedade Brasileira de Química |
publisher.none.fl_str_mv |
Sociedade Brasileira de Química |
dc.source.none.fl_str_mv |
Química Nova v.42 n.9 2019 reponame:Química Nova (Online) instname:Sociedade Brasileira de Química (SBQ) instacron:SBQ |
instname_str |
Sociedade Brasileira de Química (SBQ) |
instacron_str |
SBQ |
institution |
SBQ |
reponame_str |
Química Nova (Online) |
collection |
Química Nova (Online) |
repository.name.fl_str_mv |
Química Nova (Online) - Sociedade Brasileira de Química (SBQ) |
repository.mail.fl_str_mv |
quimicanova@sbq.org.br |
_version_ |
1750318120060321792 |