Processing of spent NiW/Al2O3 catalysts
Autor(a) principal: | |
---|---|
Data de Publicação: | 2013 |
Outros Autores: | , |
Tipo de documento: | Artigo |
Idioma: | eng |
Título da fonte: | Química Nova (Online) |
Texto Completo: | http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422013000500016 |
Resumo: | Spent oxidized (500 ºC, 5 h) commercial NiW/Al2O3 catalysts were processed using two different routes: a) fusion with NaOH (650 ºC, 1 h), the roasted mass was leached in water; b) leaching with HCl or H2SO4 (70 ºC, 1-3 h). HCl was the best leachant. In both routes, soluble tungsten was extracted at pH 1 with Alamine 336 (10 vol.% in kerosene) and stripped with 2 mol L-1 NH4OH (25 ºC, one stage, aqueous/organic ratio = 1 v/v). Tungsten was isolated as ammonium paratungstate at very high yield (> 97.5%). The elements were better separated using the acidic route. |
id |
SBQ-3_b80118406723b45ae65ea2793b16ef8f |
---|---|
oai_identifier_str |
oai:scielo:S0100-40422013000500016 |
network_acronym_str |
SBQ-3 |
network_name_str |
Química Nova (Online) |
repository_id_str |
|
spelling |
Processing of spent NiW/Al2O3 catalystsspent catalystsmetal recoveryNi-W catalystSpent oxidized (500 ºC, 5 h) commercial NiW/Al2O3 catalysts were processed using two different routes: a) fusion with NaOH (650 ºC, 1 h), the roasted mass was leached in water; b) leaching with HCl or H2SO4 (70 ºC, 1-3 h). HCl was the best leachant. In both routes, soluble tungsten was extracted at pH 1 with Alamine 336 (10 vol.% in kerosene) and stripped with 2 mol L-1 NH4OH (25 ºC, one stage, aqueous/organic ratio = 1 v/v). Tungsten was isolated as ammonium paratungstate at very high yield (> 97.5%). The elements were better separated using the acidic route.Sociedade Brasileira de Química2013-01-01info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersiontext/htmlhttp://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422013000500016Química Nova v.36 n.5 2013reponame:Química Nova (Online)instname:Sociedade Brasileira de Química (SBQ)instacron:SBQ10.1590/S0100-40422013000500016info:eu-repo/semantics/openAccessPaulino,Jéssica FrontinoAfonso,Julio CarlosCunha,José Waldemar Silva Dias daeng2013-07-18T00:00:00Zoai:scielo:S0100-40422013000500016Revistahttps://www.scielo.br/j/qn/ONGhttps://old.scielo.br/oai/scielo-oai.phpquimicanova@sbq.org.br1678-70640100-4042opendoar:2013-07-18T00:00Química Nova (Online) - Sociedade Brasileira de Química (SBQ)false |
dc.title.none.fl_str_mv |
Processing of spent NiW/Al2O3 catalysts |
title |
Processing of spent NiW/Al2O3 catalysts |
spellingShingle |
Processing of spent NiW/Al2O3 catalysts Paulino,Jéssica Frontino spent catalysts metal recovery Ni-W catalyst |
title_short |
Processing of spent NiW/Al2O3 catalysts |
title_full |
Processing of spent NiW/Al2O3 catalysts |
title_fullStr |
Processing of spent NiW/Al2O3 catalysts |
title_full_unstemmed |
Processing of spent NiW/Al2O3 catalysts |
title_sort |
Processing of spent NiW/Al2O3 catalysts |
author |
Paulino,Jéssica Frontino |
author_facet |
Paulino,Jéssica Frontino Afonso,Julio Carlos Cunha,José Waldemar Silva Dias da |
author_role |
author |
author2 |
Afonso,Julio Carlos Cunha,José Waldemar Silva Dias da |
author2_role |
author author |
dc.contributor.author.fl_str_mv |
Paulino,Jéssica Frontino Afonso,Julio Carlos Cunha,José Waldemar Silva Dias da |
dc.subject.por.fl_str_mv |
spent catalysts metal recovery Ni-W catalyst |
topic |
spent catalysts metal recovery Ni-W catalyst |
description |
Spent oxidized (500 ºC, 5 h) commercial NiW/Al2O3 catalysts were processed using two different routes: a) fusion with NaOH (650 ºC, 1 h), the roasted mass was leached in water; b) leaching with HCl or H2SO4 (70 ºC, 1-3 h). HCl was the best leachant. In both routes, soluble tungsten was extracted at pH 1 with Alamine 336 (10 vol.% in kerosene) and stripped with 2 mol L-1 NH4OH (25 ºC, one stage, aqueous/organic ratio = 1 v/v). Tungsten was isolated as ammonium paratungstate at very high yield (> 97.5%). The elements were better separated using the acidic route. |
publishDate |
2013 |
dc.date.none.fl_str_mv |
2013-01-01 |
dc.type.driver.fl_str_mv |
info:eu-repo/semantics/article |
dc.type.status.fl_str_mv |
info:eu-repo/semantics/publishedVersion |
format |
article |
status_str |
publishedVersion |
dc.identifier.uri.fl_str_mv |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422013000500016 |
url |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422013000500016 |
dc.language.iso.fl_str_mv |
eng |
language |
eng |
dc.relation.none.fl_str_mv |
10.1590/S0100-40422013000500016 |
dc.rights.driver.fl_str_mv |
info:eu-repo/semantics/openAccess |
eu_rights_str_mv |
openAccess |
dc.format.none.fl_str_mv |
text/html |
dc.publisher.none.fl_str_mv |
Sociedade Brasileira de Química |
publisher.none.fl_str_mv |
Sociedade Brasileira de Química |
dc.source.none.fl_str_mv |
Química Nova v.36 n.5 2013 reponame:Química Nova (Online) instname:Sociedade Brasileira de Química (SBQ) instacron:SBQ |
instname_str |
Sociedade Brasileira de Química (SBQ) |
instacron_str |
SBQ |
institution |
SBQ |
reponame_str |
Química Nova (Online) |
collection |
Química Nova (Online) |
repository.name.fl_str_mv |
Química Nova (Online) - Sociedade Brasileira de Química (SBQ) |
repository.mail.fl_str_mv |
quimicanova@sbq.org.br |
_version_ |
1750318114746138624 |