Influência do pré-aquecimento de resinas bulk-fill e cimentos de ionômero de vidro nas propriedades físico-mecânicas

Detalhes bibliográficos
Autor(a) principal: Lopes, Larissa Coelho Pires
Data de Publicação: 2020
Tipo de documento: Tese
Idioma: por
Título da fonte: Repositório Institucional da Universidade Estadual de Maringá (RI-UEM)
Texto Completo: http://repositorio.uem.br:8080/jspui/handle/1/6831
Resumo: Orientadora: Profª. Drª. Raquel Sano Suga Terada.
id UEM-10_0e47ee80337fe9b689b153515ceda152
oai_identifier_str oai:localhost:1/6831
network_acronym_str UEM-10
network_name_str Repositório Institucional da Universidade Estadual de Maringá (RI-UEM)
repository_id_str
spelling Influência do pré-aquecimento de resinas bulk-fill e cimentos de ionômero de vidro nas propriedades físico-mecânicasResinas compostasCimentos de ionômero de vidro (CIV)617.695Ciências da SaúdeOdontologiaOrientadora: Profª. Drª. Raquel Sano Suga Terada.Coorientadora: Profª. Drª. Renata Corrêa Pascotto.Tese (doutorado em Odontologia) - Universidade Estadual de Maringá, 2020.Um desafio frequente na prática clínica com restaurações de resina composta é conseguir um bom selamento e consequentemente, boa adaptação marginal. Para as restaurações com cimentos de ionômero de vidro (CIV), especialmente nos períodos iniciais após a mistura, o desafio é assegurar que o material atinja bons níveis de resistência mecânica. Uma das alternativas propostas para contornar esses problemas tem sido o pré-aquecimento das resinas antes da inserção do material na cavidade e o aquecimento do CIV recém-manipulado com fontes de calor. Neste contexto, o objetivo deste trabalho foi avaliar a influência do préaquecimento de resinas compostas bulk-fill e de CIV nas propriedades físico-mecânicas. Para tanto, foram realizados quatro trabalhos, sendo uma revisão sistemática e três ensaios laboratoriais. Os objetivos de cada estudo foram: 1) realizar uma revisão sistemática sobre a influência do pré-aquecimento e/ou aquecimento de materiais resinosos e ionoméricos nas propriedades físicas e mecânicas e discutir os benefícios e as formas de pré-aquecimento que têm sido realizadas; 2) avaliar o efeito do pré-aquecimento de cimentos de ionômero de vidro no tempo de estabilização (TS) das ligações químicas e na microdureza; 3) avaliar o efeito do pré-aquecimento na liberação e absorção de flúor dos CIV Equia Forte/GC e Ketac Universal/3M ESPE; 4) avaliar o comportamento de fluxo e viscoelasticidade sob tensão de cisalhamento contínuo, a microdureza e o grau de conversão de resinas compostas bulk-fill de consistência flow (BFF), em diferentes temperaturas de pré-aquecimento. Com base nos achados desses estudos, verificou-se que o pré-aquecimento de BFF e CIV é uma técnica simples, segura e com bons resultados. Com base nos resultados da revisão sistemática verifica-se que o pré-aquecimento melhora as propriedades mecânicas e físicas dos materiais resinosos e ionoméricos. Os resultados dos estudos in vitro realizados mostraram que o préaquecimento de CIV reduziu o TS para o Equia Forte, mas aumentou para o Ketac Universal, bem como aumentou significativamente a microdureza do Ketac Universal e Equia Forte. O pré-aquecimento dos CIV não alterou o padrão de liberação e absorção de flúor. Com relação ao pré-aquecimento de BFF verificou-se uma redução da viscosidade, melhora da microdureza para alguns materiais e que o procedimento não influenciou o grau de conversão em todas as profundidades da restauração. Conclui-se que as vantagens da indicação de mais uma etapa de pré-aquecimento das resinas compostas bulk-fill flow ou ionômeros de vidro ao procedimento restaurador são questionáveis. Para atingir bons resultados é necessário agilidade para que os materiais não percam calor até o momento do procedimento restaurador e cuidado para não incluir bolhas e evitar a formação de gaps, o que compromete o melhor desempenho da restauração.A frequent challenge in clinical practice with composite resin restorations is to achieve a good seal and, consequently, good marginal adaptation. For restorations with glass ionomer cements (GIC), especially in the initial periods after mixing, the challenge is to ensure that the material reaches good levels of mechanical resistance. One of the proposed alternatives to overcome these problems has been the preheating of the resins before the insertion of the material in the cavity and heating the newly GIC manipulated with heat sources. In this context, the objective of this work was to evaluate the influence of the preheating of bulk-fill and GIC composite resins on the physical-mechanical properties. For this purpose, four articles were carried out, one being a systematic review and three laboratory tests. The objectives of each study were: 1) to carry out a systematic review on the influence of the preheating and / or heating of resinous and ionomeric materials on the physical and mechanical properties and to discuss the benefits and the forms of preheating that have been carried out for resinous materials and glass ionomer cements; 2) evaluate the effect of preheating glass ionomer cements on the stabilization time (ST) of chemical bonds and on microhardness; 3) to evaluate the effect of preheating on the fluoride release and absorption of the GIC Equia Forte / GC and Ketac Universal / 3M ESPE; 4) to evaluate the behavior of flow and viscoelasticity under continuous shear stress, the microhardness and the degree of conversion of bulk-fill resins of flow consistency (BFF), at different preheating temperatures. Based on the findings of these studies, it was found that the preheating of BFF and CIV composite resins is a simple, safe technique and with good results. Based on the results of the systematic review, it appears that preheating improves the mechanical and physical properties of resin and ionomeric materials. According to the in vitro studies carried out, the following results were found: the pre-heating of GIC reduced the ST for Equia Forte, but increased for Ketac Universal, as well as significantly increased the microhardness of Ketac Universal and Equia Forte. The preheating of the GIC did not change the fluoride release and absorption pattern. Regarding the preheating of BFF, a reduction in viscosity was observed, improvement of microhardness for some materials and that the procedure did not influence the degree of conversion in all depths of the restoration. It is concluded that the advantages of indicating yet another preheating step for bulk-fill flow resins or glass ionomers still in the restorative procedure are questionable. To achieve good results, agility is required so that the materials do not lose heat until the moment of the restorative procedure and care not to include bubbles and avoid the formation of gaps, which compromises the best performance of the restoration.127 f. : il. color.Universidade Estadual de MaringáDepartamento de OdontologiaPrograma de Pós-Graduação em Odontologia IntegradaMaringá, PRCentro de Ciências da SaúdeTerada, Raquel Sano SugaPascotto, Renata CorrêaBaesso, Mauro LucianoPereira, Jefferson RicardoSoares, Carlos JoséNaufel, Fabiana ScarparoLopes, Larissa Coelho Pires2022-09-20T13:23:22Z2022-09-20T13:23:22Z2020info:eu-repo/semantics/publishedVersioninfo:eu-repo/semantics/doctoralThesisapplication/pdfLOPES, Larissa Coelho Pires. Influência do pré-aquecimento de resinas bulk-fill e cimentos de ionômero de vidro nas propriedades físico-mecânicas. 2020. 127 f. Tese (doutorado em Odontologia) - Universidade Estadual de Maringá, 2020., Maringá, PR.http://repositorio.uem.br:8080/jspui/handle/1/6831info:eu-repo/semantics/openAccessporreponame:Repositório Institucional da Universidade Estadual de Maringá (RI-UEM)instname:Universidade Estadual de Maringá (UEM)instacron:UEM2023-10-25T18:52:22Zoai:localhost:1/6831Repositório InstitucionalPUBhttp://repositorio.uem.br:8080/oai/requestopendoar:2024-04-23T14:59:46.064836Repositório Institucional da Universidade Estadual de Maringá (RI-UEM) - Universidade Estadual de Maringá (UEM)false
dc.title.none.fl_str_mv Influência do pré-aquecimento de resinas bulk-fill e cimentos de ionômero de vidro nas propriedades físico-mecânicas
title Influência do pré-aquecimento de resinas bulk-fill e cimentos de ionômero de vidro nas propriedades físico-mecânicas
spellingShingle Influência do pré-aquecimento de resinas bulk-fill e cimentos de ionômero de vidro nas propriedades físico-mecânicas
Lopes, Larissa Coelho Pires
Resinas compostas
Cimentos de ionômero de vidro (CIV)
617.695
Ciências da Saúde
Odontologia
title_short Influência do pré-aquecimento de resinas bulk-fill e cimentos de ionômero de vidro nas propriedades físico-mecânicas
title_full Influência do pré-aquecimento de resinas bulk-fill e cimentos de ionômero de vidro nas propriedades físico-mecânicas
title_fullStr Influência do pré-aquecimento de resinas bulk-fill e cimentos de ionômero de vidro nas propriedades físico-mecânicas
title_full_unstemmed Influência do pré-aquecimento de resinas bulk-fill e cimentos de ionômero de vidro nas propriedades físico-mecânicas
title_sort Influência do pré-aquecimento de resinas bulk-fill e cimentos de ionômero de vidro nas propriedades físico-mecânicas
author Lopes, Larissa Coelho Pires
author_facet Lopes, Larissa Coelho Pires
author_role author
dc.contributor.none.fl_str_mv Terada, Raquel Sano Suga
Pascotto, Renata Corrêa
Baesso, Mauro Luciano
Pereira, Jefferson Ricardo
Soares, Carlos José
Naufel, Fabiana Scarparo
dc.contributor.author.fl_str_mv Lopes, Larissa Coelho Pires
dc.subject.por.fl_str_mv Resinas compostas
Cimentos de ionômero de vidro (CIV)
617.695
Ciências da Saúde
Odontologia
topic Resinas compostas
Cimentos de ionômero de vidro (CIV)
617.695
Ciências da Saúde
Odontologia
description Orientadora: Profª. Drª. Raquel Sano Suga Terada.
publishDate 2020
dc.date.none.fl_str_mv 2020
2022-09-20T13:23:22Z
2022-09-20T13:23:22Z
dc.type.status.fl_str_mv info:eu-repo/semantics/publishedVersion
dc.type.driver.fl_str_mv info:eu-repo/semantics/doctoralThesis
format doctoralThesis
status_str publishedVersion
dc.identifier.uri.fl_str_mv LOPES, Larissa Coelho Pires. Influência do pré-aquecimento de resinas bulk-fill e cimentos de ionômero de vidro nas propriedades físico-mecânicas. 2020. 127 f. Tese (doutorado em Odontologia) - Universidade Estadual de Maringá, 2020., Maringá, PR.
http://repositorio.uem.br:8080/jspui/handle/1/6831
identifier_str_mv LOPES, Larissa Coelho Pires. Influência do pré-aquecimento de resinas bulk-fill e cimentos de ionômero de vidro nas propriedades físico-mecânicas. 2020. 127 f. Tese (doutorado em Odontologia) - Universidade Estadual de Maringá, 2020., Maringá, PR.
url http://repositorio.uem.br:8080/jspui/handle/1/6831
dc.language.iso.fl_str_mv por
language por
dc.rights.driver.fl_str_mv info:eu-repo/semantics/openAccess
eu_rights_str_mv openAccess
dc.format.none.fl_str_mv application/pdf
dc.publisher.none.fl_str_mv Universidade Estadual de Maringá
Departamento de Odontologia
Programa de Pós-Graduação em Odontologia Integrada
Maringá, PR
Centro de Ciências da Saúde
publisher.none.fl_str_mv Universidade Estadual de Maringá
Departamento de Odontologia
Programa de Pós-Graduação em Odontologia Integrada
Maringá, PR
Centro de Ciências da Saúde
dc.source.none.fl_str_mv reponame:Repositório Institucional da Universidade Estadual de Maringá (RI-UEM)
instname:Universidade Estadual de Maringá (UEM)
instacron:UEM
instname_str Universidade Estadual de Maringá (UEM)
instacron_str UEM
institution UEM
reponame_str Repositório Institucional da Universidade Estadual de Maringá (RI-UEM)
collection Repositório Institucional da Universidade Estadual de Maringá (RI-UEM)
repository.name.fl_str_mv Repositório Institucional da Universidade Estadual de Maringá (RI-UEM) - Universidade Estadual de Maringá (UEM)
repository.mail.fl_str_mv
_version_ 1801841441721286656