Secondary recrystallization characteristics of 3%Si grain-oriented electrical steel.

Detalhes bibliográficos
Autor(a) principal: Cardoso, Afonso Vaz de Mello
Data de Publicação: 2018
Outros Autores: Paolinelli, Sebastião da Costa, Silveira, Carolina Cesconetto, Cota, André Barros
Tipo de documento: Artigo
Idioma: eng
Título da fonte: Repositório Institucional da UFOP
Texto Completo: http://www.repositorio.ufop.br/handle/123456789/11468
https://doi.org/10.1016/j.jmrt.2017.12.002
Resumo: A secondary recrystallization Lab study focusing on the secondary recrystallization temper- ature and magnetic properties was carried out on cold rolling industrial samples of 3%Si grain-oriented electrical steel produced by low slab reheating temperature technology. The results showed a secondary recrystallization temperature, determined by the observed grain size change, of 1080 ◦C with annealing interruption and of 1060 ◦C in annealing for 50 h at constant temperature. In addition, the best set of magnetic properties, the higher induction and the lower core loss values, was achieved by annealing the samples during 50 h at 1070 ◦C constant temperature.
id UFOP_4fcddbd1458ba826be1ae3d88ed50496
oai_identifier_str oai:repositorio.ufop.br:123456789/11468
network_acronym_str UFOP
network_name_str Repositório Institucional da UFOP
repository_id_str 3233
spelling Secondary recrystallization characteristics of 3%Si grain-oriented electrical steel.Grain-oriented steelMagnetic propertiesA secondary recrystallization Lab study focusing on the secondary recrystallization temper- ature and magnetic properties was carried out on cold rolling industrial samples of 3%Si grain-oriented electrical steel produced by low slab reheating temperature technology. The results showed a secondary recrystallization temperature, determined by the observed grain size change, of 1080 ◦C with annealing interruption and of 1060 ◦C in annealing for 50 h at constant temperature. In addition, the best set of magnetic properties, the higher induction and the lower core loss values, was achieved by annealing the samples during 50 h at 1070 ◦C constant temperature.2019-06-06T18:16:06Z2019-06-06T18:16:06Z2018info:eu-repo/semantics/publishedVersioninfo:eu-repo/semantics/articleapplication/pdfCARDOSO, A. F. de M. et al. Secondary recrystallization characteristics of 3%Si grain-oriented electrical steel. Journal of Materials Research and Technology - JMR&T, v. 8, n. 1, p. 240-245, jan./mar. 2018. Disponível em: <https://www.sciencedirect.com/science/article/pii/S2238785417301990>. Acesso em: 19 mar. 2019.2238-7854http://www.repositorio.ufop.br/handle/123456789/11468https://doi.org/10.1016/j.jmrt.2017.12.002This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/). Fonte: o próprio artigo.info:eu-repo/semantics/openAccessCardoso, Afonso Vaz de MelloPaolinelli, Sebastião da CostaSilveira, Carolina CesconettoCota, André Barrosengreponame:Repositório Institucional da UFOPinstname:Universidade Federal de Ouro Preto (UFOP)instacron:UFOP2019-06-06T18:16:06Zoai:repositorio.ufop.br:123456789/11468Repositório InstitucionalPUBhttp://www.repositorio.ufop.br/oai/requestrepositorio@ufop.edu.bropendoar:32332019-06-06T18:16:06Repositório Institucional da UFOP - Universidade Federal de Ouro Preto (UFOP)false
dc.title.none.fl_str_mv Secondary recrystallization characteristics of 3%Si grain-oriented electrical steel.
title Secondary recrystallization characteristics of 3%Si grain-oriented electrical steel.
spellingShingle Secondary recrystallization characteristics of 3%Si grain-oriented electrical steel.
Cardoso, Afonso Vaz de Mello
Grain-oriented steel
Magnetic properties
title_short Secondary recrystallization characteristics of 3%Si grain-oriented electrical steel.
title_full Secondary recrystallization characteristics of 3%Si grain-oriented electrical steel.
title_fullStr Secondary recrystallization characteristics of 3%Si grain-oriented electrical steel.
title_full_unstemmed Secondary recrystallization characteristics of 3%Si grain-oriented electrical steel.
title_sort Secondary recrystallization characteristics of 3%Si grain-oriented electrical steel.
author Cardoso, Afonso Vaz de Mello
author_facet Cardoso, Afonso Vaz de Mello
Paolinelli, Sebastião da Costa
Silveira, Carolina Cesconetto
Cota, André Barros
author_role author
author2 Paolinelli, Sebastião da Costa
Silveira, Carolina Cesconetto
Cota, André Barros
author2_role author
author
author
dc.contributor.author.fl_str_mv Cardoso, Afonso Vaz de Mello
Paolinelli, Sebastião da Costa
Silveira, Carolina Cesconetto
Cota, André Barros
dc.subject.por.fl_str_mv Grain-oriented steel
Magnetic properties
topic Grain-oriented steel
Magnetic properties
description A secondary recrystallization Lab study focusing on the secondary recrystallization temper- ature and magnetic properties was carried out on cold rolling industrial samples of 3%Si grain-oriented electrical steel produced by low slab reheating temperature technology. The results showed a secondary recrystallization temperature, determined by the observed grain size change, of 1080 ◦C with annealing interruption and of 1060 ◦C in annealing for 50 h at constant temperature. In addition, the best set of magnetic properties, the higher induction and the lower core loss values, was achieved by annealing the samples during 50 h at 1070 ◦C constant temperature.
publishDate 2018
dc.date.none.fl_str_mv 2018
2019-06-06T18:16:06Z
2019-06-06T18:16:06Z
dc.type.status.fl_str_mv info:eu-repo/semantics/publishedVersion
dc.type.driver.fl_str_mv info:eu-repo/semantics/article
format article
status_str publishedVersion
dc.identifier.uri.fl_str_mv CARDOSO, A. F. de M. et al. Secondary recrystallization characteristics of 3%Si grain-oriented electrical steel. Journal of Materials Research and Technology - JMR&T, v. 8, n. 1, p. 240-245, jan./mar. 2018. Disponível em: <https://www.sciencedirect.com/science/article/pii/S2238785417301990>. Acesso em: 19 mar. 2019.
2238-7854
http://www.repositorio.ufop.br/handle/123456789/11468
https://doi.org/10.1016/j.jmrt.2017.12.002
identifier_str_mv CARDOSO, A. F. de M. et al. Secondary recrystallization characteristics of 3%Si grain-oriented electrical steel. Journal of Materials Research and Technology - JMR&T, v. 8, n. 1, p. 240-245, jan./mar. 2018. Disponível em: <https://www.sciencedirect.com/science/article/pii/S2238785417301990>. Acesso em: 19 mar. 2019.
2238-7854
url http://www.repositorio.ufop.br/handle/123456789/11468
https://doi.org/10.1016/j.jmrt.2017.12.002
dc.language.iso.fl_str_mv eng
language eng
dc.rights.driver.fl_str_mv info:eu-repo/semantics/openAccess
eu_rights_str_mv openAccess
dc.format.none.fl_str_mv application/pdf
dc.source.none.fl_str_mv reponame:Repositório Institucional da UFOP
instname:Universidade Federal de Ouro Preto (UFOP)
instacron:UFOP
instname_str Universidade Federal de Ouro Preto (UFOP)
instacron_str UFOP
institution UFOP
reponame_str Repositório Institucional da UFOP
collection Repositório Institucional da UFOP
repository.name.fl_str_mv Repositório Institucional da UFOP - Universidade Federal de Ouro Preto (UFOP)
repository.mail.fl_str_mv repositorio@ufop.edu.br
_version_ 1813002812401909760