Influência da espessura da camada de opaco na capacidade de mascaramento de metalocerâmicas

Detalhes bibliográficos
Autor(a) principal: Pieper, Cari Maristela
Data de Publicação: 2012
Tipo de documento: Dissertação
Idioma: por
Título da fonte: Repositório Institucional da UFPel - Guaiaca
Texto Completo: http://repositorio.ufpel.edu.br/handle/ri/2275
Resumo: The aim of this study was to evaluate the ability of two ceramic opaque masking applied in different thicknesses in a metallic substrate. 80 Ni-Cr (High Bond) metalic discs were fabricated, each with 1.6 mm diameter and 1 mm thickness, by lost wax technique. After disks obtaining, they were divided into 8 groups (n = 10) and opaque ceramic (Noritake) "paste" (groups 1 to 4) and "powder" (groups 5 to 8) was applied with a camel hair brush and distilled water. The opaque layers were machined with aluminum oxide burs to achieve the following thickness: G1 = G5 and 0.10 mm thick; G2 and G6 = 0.15 mm; G3 and G7 = 0.20 mm and G4 and G8 = 0.30 mm thick. Than opaque dentin ceramic was applied (two sintering cicles, totaling 0.7 mm) and glazed. The color was evaluated with the aid of a portable spectrocolorimeter (Konica - Minolta CR-10), which registered the color of specimens in the CIE L*a*b* scale. The absolute values of L *, a * and b * were statistically analyzed as isolated variables.The ΔE were also analyzed, considering the mean values of L * a * b * in the control group (G4) as reference values. Once data showed normality and homogeneity, it were applied 2-way ANOVA and Tukey s complementary test, when needed, with p < 5%. Results: Powder opaque presented statistically significant greater values in (L*) and (ΔE) and the reverse happened to other two variables. Analysing opaque thickness, values may be grouped as followed: (L*) variable: (0,10mm = 0,15mm) < (0,20mm = 0,30mm); (a*) variable: (0,10mm) < (0,15mm = 0,20mm) < (0,30mm); (b*) variable showed no statistically significant differences; (ΔE) variable: (0,10mm) < (0,15mm = 0,20mm = 0,30mms). It could be concluded that paste and powder opaque have different behavior and all thickness, except 0,10 mm, may be used without significant color change
id UFPL_5dca9c87f868a5683ac4ea292f92740b
oai_identifier_str oai:guaiaca.ufpel.edu.br:123456789/2275
network_acronym_str UFPL
network_name_str Repositório Institucional da UFPel - Guaiaca
repository_id_str
spelling 2014-08-20T14:30:14Z2014-01-242014-08-20T14:30:14Z2012-12-19PIEPER, Cari Maristela. Capacity opaque masking layer in thicknesses of metal laminated ceramics application. 2012. 58 f. Dissertação (Mestrado em Odontologia) - Universidade Federal de Pelotas, Pelotas, 2012.http://repositorio.ufpel.edu.br/handle/ri/2275The aim of this study was to evaluate the ability of two ceramic opaque masking applied in different thicknesses in a metallic substrate. 80 Ni-Cr (High Bond) metalic discs were fabricated, each with 1.6 mm diameter and 1 mm thickness, by lost wax technique. After disks obtaining, they were divided into 8 groups (n = 10) and opaque ceramic (Noritake) "paste" (groups 1 to 4) and "powder" (groups 5 to 8) was applied with a camel hair brush and distilled water. The opaque layers were machined with aluminum oxide burs to achieve the following thickness: G1 = G5 and 0.10 mm thick; G2 and G6 = 0.15 mm; G3 and G7 = 0.20 mm and G4 and G8 = 0.30 mm thick. Than opaque dentin ceramic was applied (two sintering cicles, totaling 0.7 mm) and glazed. The color was evaluated with the aid of a portable spectrocolorimeter (Konica - Minolta CR-10), which registered the color of specimens in the CIE L*a*b* scale. The absolute values of L *, a * and b * were statistically analyzed as isolated variables.The ΔE were also analyzed, considering the mean values of L * a * b * in the control group (G4) as reference values. Once data showed normality and homogeneity, it were applied 2-way ANOVA and Tukey s complementary test, when needed, with p < 5%. Results: Powder opaque presented statistically significant greater values in (L*) and (ΔE) and the reverse happened to other two variables. Analysing opaque thickness, values may be grouped as followed: (L*) variable: (0,10mm = 0,15mm) < (0,20mm = 0,30mm); (a*) variable: (0,10mm) < (0,15mm = 0,20mm) < (0,30mm); (b*) variable showed no statistically significant differences; (ΔE) variable: (0,10mm) < (0,15mm = 0,20mm = 0,30mms). It could be concluded that paste and powder opaque have different behavior and all thickness, except 0,10 mm, may be used without significant color changeO objetivo deste estudo foi avaliar a capacidade de mascaramento de duas cerâmicas opacas aplicadas em espessuras diferentes num substrato metálico. Para isso foram confeccionados 80 discos metálicos de Ni-Cr (High Bond) com 16 mm de diâmetro e 1mm de espessura, através da técnica da cera perdida. Após a obtenção dos discos estes foram divididos em 8 grupos (n=10) e foi aplicada a cerâmica opaca (Noritake) em pasta (grupos de 1 à 4) e em pó (grupos de 5 à 8) com pincel de pêlo de camelo e água destilada. As camadas opacas foram usinadas com pontas de óxido de alumínio até atingirem as seguintes espessuras: G1 e G5 = 0,10mm de espessura; G2 e G6 = 0,15mm; G3 e G7 = 0,20mm e G4 e G8 = 0,30mm de espessura. Após, foi aplicada cerâmica de dentina opaca (em dois ciclos de sinterização totalizando 0,7mm), e em seguida à sinterização foi realizado o glaze final.A avaliação da cor foi realizada com o auxílio do Espectrocolorímetro portátil (Konica - Minolta CR-10), que registrou a cor dos 80 corpos de prova metalocerâmicos nos eixos da escala CIE - L*, a* b* após o ciclo de glaze. Os valores absolutos de L*, a* e b* dos grupos foram analisados estatísticamente como variáveis isoladas. Também foi analisado o valor da variável ΔE, sendo que os valores médios de L* a* e b* do grupo controle (G4) foram considerados como os valores de referência para os cálculos do Δa, Δb, ΔL e ΔE dos demais grupos. Após constatada normalidade e homogeneidade dos dados foi aplicada análise de variância para dois fatores de variação (2-way ANOVA) e teste complementar de Tukey ambos para p<5%. Resultados: O opaco em pó apresentou valores maiores estaticamente significantes nas variáveis (L*) e (ΔE), ocorrendo o inverso nas outras duas variáveis.Quanto à espessura de opaco, os valores podem ser agrupados da seguinte forma, segundo os testes complementares aplicados: variável (L*): (0,10mm = 0,15mm) < (0,20mm = 0,30mm); variável (a*): (0,10mm) < (0,15mm = 0,20mm) < (0,30mm); variável (b*): não houveram diferenças estatisticamente significantes; variável (ΔE): (0,10mm) < (0,15mm = 0,20mm = 0,30mm). Conclui-se que houve diferença entre os tipos de opaco em pasta e em pó e que todas as espessuras testadas, exceto a de 0,10 mm, podem ser usadas sem alteração significativa da corapplication/pdfporUniversidade Federal de PelotasPrograma de Pós-Graduação em OdontologiaUFPelBROdontologiaLigas metalo-cerâmicasCerâmica opacaOpacidadeMetal-ceramic alloysCeramic opaqueOpacityCNPQ::CIENCIAS DA SAUDE::ODONTOLOGIAInfluência da espessura da camada de opaco na capacidade de mascaramento de metalocerâmicasCapacity opaque masking layer in thicknesses of metal laminated ceramics applicationinfo:eu-repo/semantics/publishedVersioninfo:eu-repo/semantics/masterThesishttp://lattes.cnpq.br/3907489657746199Waldemarin, Renato Fabrício de Andradehttp://lattes.cnpq.br/6542284107758719Camacho, Guilherme BriãoPieper, Cari Maristelainfo:eu-repo/semantics/openAccessreponame:Repositório Institucional da UFPel - Guaiacainstname:Universidade Federal de Pelotas (UFPEL)instacron:UFPELORIGINALDissertacao_Cari_Maristela_Pieper.pdfapplication/pdf422459http://guaiaca.ufpel.edu.br/xmlui/bitstream/123456789/2275/1/Dissertacao_Cari_Maristela_Pieper.pdf06736de352d724ef840d5461683237cdMD51open accessTEXTDissertacao_Cari_Maristela_Pieper.pdf.txtDissertacao_Cari_Maristela_Pieper.pdf.txtExtracted Texttext/plain83343http://guaiaca.ufpel.edu.br/xmlui/bitstream/123456789/2275/2/Dissertacao_Cari_Maristela_Pieper.pdf.txt814da1ea26691ca0aa498359603bf004MD52open accessTHUMBNAILDissertacao_Cari_Maristela_Pieper.pdf.jpgDissertacao_Cari_Maristela_Pieper.pdf.jpgGenerated Thumbnailimage/jpeg1911http://guaiaca.ufpel.edu.br/xmlui/bitstream/123456789/2275/3/Dissertacao_Cari_Maristela_Pieper.pdf.jpg81595dc7ece7b79c1a55f0f96dfc87b3MD53open access123456789/22752019-09-19 08:50:16.663open accessoai:guaiaca.ufpel.edu.br:123456789/2275Repositório InstitucionalPUBhttp://repositorio.ufpel.edu.br/oai/requestrippel@ufpel.edu.br || repositorio@ufpel.edu.br || aline.batista@ufpel.edu.bropendoar:2019-09-19T11:50:16Repositório Institucional da UFPel - Guaiaca - Universidade Federal de Pelotas (UFPEL)false
dc.title.por.fl_str_mv Influência da espessura da camada de opaco na capacidade de mascaramento de metalocerâmicas
dc.title.alternative.eng.fl_str_mv Capacity opaque masking layer in thicknesses of metal laminated ceramics application
title Influência da espessura da camada de opaco na capacidade de mascaramento de metalocerâmicas
spellingShingle Influência da espessura da camada de opaco na capacidade de mascaramento de metalocerâmicas
Pieper, Cari Maristela
Ligas metalo-cerâmicas
Cerâmica opaca
Opacidade
Metal-ceramic alloys
Ceramic opaque
Opacity
CNPQ::CIENCIAS DA SAUDE::ODONTOLOGIA
title_short Influência da espessura da camada de opaco na capacidade de mascaramento de metalocerâmicas
title_full Influência da espessura da camada de opaco na capacidade de mascaramento de metalocerâmicas
title_fullStr Influência da espessura da camada de opaco na capacidade de mascaramento de metalocerâmicas
title_full_unstemmed Influência da espessura da camada de opaco na capacidade de mascaramento de metalocerâmicas
title_sort Influência da espessura da camada de opaco na capacidade de mascaramento de metalocerâmicas
author Pieper, Cari Maristela
author_facet Pieper, Cari Maristela
author_role author
dc.contributor.authorLattes.por.fl_str_mv http://lattes.cnpq.br/3907489657746199
dc.contributor.advisor-co1.fl_str_mv Waldemarin, Renato Fabrício de Andrade
dc.contributor.advisor-co1Lattes.fl_str_mv http://lattes.cnpq.br/6542284107758719
dc.contributor.advisor1.fl_str_mv Camacho, Guilherme Brião
dc.contributor.author.fl_str_mv Pieper, Cari Maristela
contributor_str_mv Waldemarin, Renato Fabrício de Andrade
Camacho, Guilherme Brião
dc.subject.por.fl_str_mv Ligas metalo-cerâmicas
Cerâmica opaca
Opacidade
topic Ligas metalo-cerâmicas
Cerâmica opaca
Opacidade
Metal-ceramic alloys
Ceramic opaque
Opacity
CNPQ::CIENCIAS DA SAUDE::ODONTOLOGIA
dc.subject.eng.fl_str_mv Metal-ceramic alloys
Ceramic opaque
Opacity
dc.subject.cnpq.fl_str_mv CNPQ::CIENCIAS DA SAUDE::ODONTOLOGIA
description The aim of this study was to evaluate the ability of two ceramic opaque masking applied in different thicknesses in a metallic substrate. 80 Ni-Cr (High Bond) metalic discs were fabricated, each with 1.6 mm diameter and 1 mm thickness, by lost wax technique. After disks obtaining, they were divided into 8 groups (n = 10) and opaque ceramic (Noritake) "paste" (groups 1 to 4) and "powder" (groups 5 to 8) was applied with a camel hair brush and distilled water. The opaque layers were machined with aluminum oxide burs to achieve the following thickness: G1 = G5 and 0.10 mm thick; G2 and G6 = 0.15 mm; G3 and G7 = 0.20 mm and G4 and G8 = 0.30 mm thick. Than opaque dentin ceramic was applied (two sintering cicles, totaling 0.7 mm) and glazed. The color was evaluated with the aid of a portable spectrocolorimeter (Konica - Minolta CR-10), which registered the color of specimens in the CIE L*a*b* scale. The absolute values of L *, a * and b * were statistically analyzed as isolated variables.The ΔE were also analyzed, considering the mean values of L * a * b * in the control group (G4) as reference values. Once data showed normality and homogeneity, it were applied 2-way ANOVA and Tukey s complementary test, when needed, with p < 5%. Results: Powder opaque presented statistically significant greater values in (L*) and (ΔE) and the reverse happened to other two variables. Analysing opaque thickness, values may be grouped as followed: (L*) variable: (0,10mm = 0,15mm) < (0,20mm = 0,30mm); (a*) variable: (0,10mm) < (0,15mm = 0,20mm) < (0,30mm); (b*) variable showed no statistically significant differences; (ΔE) variable: (0,10mm) < (0,15mm = 0,20mm = 0,30mms). It could be concluded that paste and powder opaque have different behavior and all thickness, except 0,10 mm, may be used without significant color change
publishDate 2012
dc.date.issued.fl_str_mv 2012-12-19
dc.date.accessioned.fl_str_mv 2014-08-20T14:30:14Z
dc.date.available.fl_str_mv 2014-01-24
2014-08-20T14:30:14Z
dc.type.status.fl_str_mv info:eu-repo/semantics/publishedVersion
dc.type.driver.fl_str_mv info:eu-repo/semantics/masterThesis
format masterThesis
status_str publishedVersion
dc.identifier.citation.fl_str_mv PIEPER, Cari Maristela. Capacity opaque masking layer in thicknesses of metal laminated ceramics application. 2012. 58 f. Dissertação (Mestrado em Odontologia) - Universidade Federal de Pelotas, Pelotas, 2012.
dc.identifier.uri.fl_str_mv http://repositorio.ufpel.edu.br/handle/ri/2275
identifier_str_mv PIEPER, Cari Maristela. Capacity opaque masking layer in thicknesses of metal laminated ceramics application. 2012. 58 f. Dissertação (Mestrado em Odontologia) - Universidade Federal de Pelotas, Pelotas, 2012.
url http://repositorio.ufpel.edu.br/handle/ri/2275
dc.language.iso.fl_str_mv por
language por
dc.rights.driver.fl_str_mv info:eu-repo/semantics/openAccess
eu_rights_str_mv openAccess
dc.format.none.fl_str_mv application/pdf
dc.publisher.none.fl_str_mv Universidade Federal de Pelotas
dc.publisher.program.fl_str_mv Programa de Pós-Graduação em Odontologia
dc.publisher.initials.fl_str_mv UFPel
dc.publisher.country.fl_str_mv BR
dc.publisher.department.fl_str_mv Odontologia
publisher.none.fl_str_mv Universidade Federal de Pelotas
dc.source.none.fl_str_mv reponame:Repositório Institucional da UFPel - Guaiaca
instname:Universidade Federal de Pelotas (UFPEL)
instacron:UFPEL
instname_str Universidade Federal de Pelotas (UFPEL)
instacron_str UFPEL
institution UFPEL
reponame_str Repositório Institucional da UFPel - Guaiaca
collection Repositório Institucional da UFPel - Guaiaca
bitstream.url.fl_str_mv http://guaiaca.ufpel.edu.br/xmlui/bitstream/123456789/2275/1/Dissertacao_Cari_Maristela_Pieper.pdf
http://guaiaca.ufpel.edu.br/xmlui/bitstream/123456789/2275/2/Dissertacao_Cari_Maristela_Pieper.pdf.txt
http://guaiaca.ufpel.edu.br/xmlui/bitstream/123456789/2275/3/Dissertacao_Cari_Maristela_Pieper.pdf.jpg
bitstream.checksum.fl_str_mv 06736de352d724ef840d5461683237cd
814da1ea26691ca0aa498359603bf004
81595dc7ece7b79c1a55f0f96dfc87b3
bitstream.checksumAlgorithm.fl_str_mv MD5
MD5
MD5
repository.name.fl_str_mv Repositório Institucional da UFPel - Guaiaca - Universidade Federal de Pelotas (UFPEL)
repository.mail.fl_str_mv rippel@ufpel.edu.br || repositorio@ufpel.edu.br || aline.batista@ufpel.edu.br
_version_ 1813710136126996480