Avaliação da resistência ao desgaste abrasivo de risers flexíveis proposição de nova metodologia de teste
Autor(a) principal: | |
---|---|
Data de Publicação: | 2005 |
Tipo de documento: | Dissertação |
Idioma: | por |
Título da fonte: | Repositório Institucional da UFU |
Texto Completo: | https://repositorio.ufu.br/handle/123456789/15032 |
Resumo: | The oil and gas extraction in deep waters by Petrobras has been expanded progressively in the recent years. In this condition, oil and gas can be extracted by Jacket type and semi-submersible platforms, which are connected to the wells through flexible risers. These components are constituted of a multilayer system with internal and external coatings made of polymers. On inspection of these risers, scratches and a significant reduction of the riser protection layer were observed. These damages were found to be related to the relative movement of the pipe in the area of the touchdown point (TDP). In order to reduce this problem the risers have being coated externally with plaques of polyurethane. High chemical inertia and good mechanical and abrasion resistance characterize these materials. Besides, they allow the riser to have a good flexibility. Thus, the abrasive wear of these risers was reduced. However, optimizations still must be reached. Currently, the abrasive wear resistance of these materials is evaluated by means of abrasive wear tests according to the DIN 53.516 norm and the single-pass scratching technique, both at a temperature of 4ºC. The latter one is appropriate for testing polymeric riser protections but it does not simulate the repetitive action of hard particles acting against the plaques. In the present work, a new test rig for abrasive wear testing is presented, which is based on multiple interactions between indenters and plaques. So, the deep water wear conditions were simulated and the wear micromechanisms of different polyurethane materials were observed to be similar to those of field application. The wear rate results showed that wear in these materials is basically due to microcracking. It was also noticed that materials with a good wear performance have a high tearing elongation and strength and a high resilience. A correlation between abrasive wear and mechanical properties of five different types of polyurethane was proposed. The obtained equation showed no linear relation with these results, suggesting that terms of higher degree may be important. |
id |
UFU_aa2af1a8609e4e8e06a0001e9a4f49bf |
---|---|
oai_identifier_str |
oai:repositorio.ufu.br:123456789/15032 |
network_acronym_str |
UFU |
network_name_str |
Repositório Institucional da UFU |
repository_id_str |
|
spelling |
Avaliação da resistência ao desgaste abrasivo de risers flexíveis proposição de nova metodologia de testeAbrasive Wear Resistance of Flexible Riser Protection Layers - Proposal of a New Test MethodologyDesgaste abrasivoPolímerosLinhas flexíveisPropriedades mecânicasPetróleo TubulaçõesDesgaste MecânicoTribologiaAbrasive wearPolymersFlexible risersMechanical propertiesCNPQ::ENGENHARIAS::ENGENHARIA MECANICAThe oil and gas extraction in deep waters by Petrobras has been expanded progressively in the recent years. In this condition, oil and gas can be extracted by Jacket type and semi-submersible platforms, which are connected to the wells through flexible risers. These components are constituted of a multilayer system with internal and external coatings made of polymers. On inspection of these risers, scratches and a significant reduction of the riser protection layer were observed. These damages were found to be related to the relative movement of the pipe in the area of the touchdown point (TDP). In order to reduce this problem the risers have being coated externally with plaques of polyurethane. High chemical inertia and good mechanical and abrasion resistance characterize these materials. Besides, they allow the riser to have a good flexibility. Thus, the abrasive wear of these risers was reduced. However, optimizations still must be reached. Currently, the abrasive wear resistance of these materials is evaluated by means of abrasive wear tests according to the DIN 53.516 norm and the single-pass scratching technique, both at a temperature of 4ºC. The latter one is appropriate for testing polymeric riser protections but it does not simulate the repetitive action of hard particles acting against the plaques. In the present work, a new test rig for abrasive wear testing is presented, which is based on multiple interactions between indenters and plaques. So, the deep water wear conditions were simulated and the wear micromechanisms of different polyurethane materials were observed to be similar to those of field application. The wear rate results showed that wear in these materials is basically due to microcracking. It was also noticed that materials with a good wear performance have a high tearing elongation and strength and a high resilience. A correlation between abrasive wear and mechanical properties of five different types of polyurethane was proposed. The obtained equation showed no linear relation with these results, suggesting that terms of higher degree may be important.Mestre em Engenharia MecânicaNos últimos anos, a extração de petróleo em águas profundas pela Petrobras tem sido expandida progressivamente. Uma das formas de extração do petróleo nessa condição é através de plataformas móveis, que são conectadas aos poços através de linhas flexíveis, também chamadas de risers. Esses componentes são constituídos por um complexo sistema de camadas concêntricas, sendo os revestimentos (interno e externo) confeccionados em polímeros. Recentemente, constatou-se que, no ponto de início do contato da tubulação com o fundo do mar (Touch Down Point - TDP), as linhas flexíveis experimentam um progressivo desgaste por abrasão. Para reduzir esse problema, esses componentes vêm sendo revestidos externamente com luvas bipartidas em poliuretano. Estes revestimentos são caracterizados por elevada inércia química, boa resistência mecânica, aliadas à flexibilidade necessária à estrutura. Assim, o desgaste abrasivo dessas linhas foi reduzido, necessitando, todavia, de otimizações adicionais. Atualmente, a avaliação do desempenho destes materiais vem sendo feita através de ensaios de desgaste abrasivo normatizados pela DIN 53.516 e de ensaios de esclerometria pendular, ambos a 4ºC. No presente trabalho, foi desenvolvido um equipamento e uma metodologia de ensaio de desgaste abrasivo, baseada no princípio da esclerometria pendular, capaz de facilitar a seleção e classificação de materiais para essa aplicação. As condições de desgaste existentes no fundo do mar foram simuladas reproduzindo satisfatoriamente os micromecanismos de desgaste observados na prática. A falha nesses materiais é basicamente por microtrincas, e muito provavelmente, propriedades que reprimam esse fenômeno, colaboram para uma maior resistência ao desgaste abrasivo. Pôde-se notar que materiais que têm um bom desempenho ao desgaste abrasivo têm uma boa capacidade de alongamento durante o rasgo e uma alta resiliência, somados a uma boa resistência ao rasgamento. Propôs-se, ainda, uma correlação entre desgaste abrasivo e as respectivas propriedades mecânicas de cinco tipos de poliuretanos. A equação obtida mostrou não existir uma relação linear entre esses resultados.Universidade Federal de UberlândiaBRPrograma de Pós-graduação em Engenharia MecânicaEngenhariasUFUFranco, Sinésio Domingueshttp://buscatextual.cnpq.br/buscatextual/visualizacv.do?id=K4786105Z3Mello, José Daniel Biasoli dehttp://buscatextual.cnpq.br/buscatextual/visualizacv.do?id=K4783817J1Meniconi, Luiz Cláudio de Marcohttp://buscatextual.cnpq.br/buscatextual/visualizacv.do?id=K4706618P6Moraes, Juliano Oseias de2016-06-22T18:41:13Z2007-10-252016-06-22T18:41:13Z2005-09-27info:eu-repo/semantics/publishedVersioninfo:eu-repo/semantics/masterThesisapplication/pdfapplication/zipapplication/pdfapplication/octet-streamapplication/octet-streamapplication/octet-streamapplication/octet-streamMORAES, Juliano Oseias de. Abrasive Wear Resistance of Flexible Riser Protection Layers - Proposal of a New Test Methodology. 2005. 76 f. Dissertação (Mestrado em Engenharias) - Universidade Federal de Uberlândia, Uberlândia, 2005.https://repositorio.ufu.br/handle/123456789/15032porinfo:eu-repo/semantics/openAccessreponame:Repositório Institucional da UFUinstname:Universidade Federal de Uberlândia (UFU)instacron:UFU2016-06-23T07:00:21Zoai:repositorio.ufu.br:123456789/15032Repositório InstitucionalONGhttp://repositorio.ufu.br/oai/requestdiinf@dirbi.ufu.bropendoar:2016-06-23T07:00:21Repositório Institucional da UFU - Universidade Federal de Uberlândia (UFU)false |
dc.title.none.fl_str_mv |
Avaliação da resistência ao desgaste abrasivo de risers flexíveis proposição de nova metodologia de teste Abrasive Wear Resistance of Flexible Riser Protection Layers - Proposal of a New Test Methodology |
title |
Avaliação da resistência ao desgaste abrasivo de risers flexíveis proposição de nova metodologia de teste |
spellingShingle |
Avaliação da resistência ao desgaste abrasivo de risers flexíveis proposição de nova metodologia de teste Moraes, Juliano Oseias de Desgaste abrasivo Polímeros Linhas flexíveis Propriedades mecânicas Petróleo Tubulações Desgaste Mecânico Tribologia Abrasive wear Polymers Flexible risers Mechanical properties CNPQ::ENGENHARIAS::ENGENHARIA MECANICA |
title_short |
Avaliação da resistência ao desgaste abrasivo de risers flexíveis proposição de nova metodologia de teste |
title_full |
Avaliação da resistência ao desgaste abrasivo de risers flexíveis proposição de nova metodologia de teste |
title_fullStr |
Avaliação da resistência ao desgaste abrasivo de risers flexíveis proposição de nova metodologia de teste |
title_full_unstemmed |
Avaliação da resistência ao desgaste abrasivo de risers flexíveis proposição de nova metodologia de teste |
title_sort |
Avaliação da resistência ao desgaste abrasivo de risers flexíveis proposição de nova metodologia de teste |
author |
Moraes, Juliano Oseias de |
author_facet |
Moraes, Juliano Oseias de |
author_role |
author |
dc.contributor.none.fl_str_mv |
Franco, Sinésio Domingues http://buscatextual.cnpq.br/buscatextual/visualizacv.do?id=K4786105Z3 Mello, José Daniel Biasoli de http://buscatextual.cnpq.br/buscatextual/visualizacv.do?id=K4783817J1 Meniconi, Luiz Cláudio de Marco http://buscatextual.cnpq.br/buscatextual/visualizacv.do?id=K4706618P6 |
dc.contributor.author.fl_str_mv |
Moraes, Juliano Oseias de |
dc.subject.por.fl_str_mv |
Desgaste abrasivo Polímeros Linhas flexíveis Propriedades mecânicas Petróleo Tubulações Desgaste Mecânico Tribologia Abrasive wear Polymers Flexible risers Mechanical properties CNPQ::ENGENHARIAS::ENGENHARIA MECANICA |
topic |
Desgaste abrasivo Polímeros Linhas flexíveis Propriedades mecânicas Petróleo Tubulações Desgaste Mecânico Tribologia Abrasive wear Polymers Flexible risers Mechanical properties CNPQ::ENGENHARIAS::ENGENHARIA MECANICA |
description |
The oil and gas extraction in deep waters by Petrobras has been expanded progressively in the recent years. In this condition, oil and gas can be extracted by Jacket type and semi-submersible platforms, which are connected to the wells through flexible risers. These components are constituted of a multilayer system with internal and external coatings made of polymers. On inspection of these risers, scratches and a significant reduction of the riser protection layer were observed. These damages were found to be related to the relative movement of the pipe in the area of the touchdown point (TDP). In order to reduce this problem the risers have being coated externally with plaques of polyurethane. High chemical inertia and good mechanical and abrasion resistance characterize these materials. Besides, they allow the riser to have a good flexibility. Thus, the abrasive wear of these risers was reduced. However, optimizations still must be reached. Currently, the abrasive wear resistance of these materials is evaluated by means of abrasive wear tests according to the DIN 53.516 norm and the single-pass scratching technique, both at a temperature of 4ºC. The latter one is appropriate for testing polymeric riser protections but it does not simulate the repetitive action of hard particles acting against the plaques. In the present work, a new test rig for abrasive wear testing is presented, which is based on multiple interactions between indenters and plaques. So, the deep water wear conditions were simulated and the wear micromechanisms of different polyurethane materials were observed to be similar to those of field application. The wear rate results showed that wear in these materials is basically due to microcracking. It was also noticed that materials with a good wear performance have a high tearing elongation and strength and a high resilience. A correlation between abrasive wear and mechanical properties of five different types of polyurethane was proposed. The obtained equation showed no linear relation with these results, suggesting that terms of higher degree may be important. |
publishDate |
2005 |
dc.date.none.fl_str_mv |
2005-09-27 2007-10-25 2016-06-22T18:41:13Z 2016-06-22T18:41:13Z |
dc.type.status.fl_str_mv |
info:eu-repo/semantics/publishedVersion |
dc.type.driver.fl_str_mv |
info:eu-repo/semantics/masterThesis |
format |
masterThesis |
status_str |
publishedVersion |
dc.identifier.uri.fl_str_mv |
MORAES, Juliano Oseias de. Abrasive Wear Resistance of Flexible Riser Protection Layers - Proposal of a New Test Methodology. 2005. 76 f. Dissertação (Mestrado em Engenharias) - Universidade Federal de Uberlândia, Uberlândia, 2005. https://repositorio.ufu.br/handle/123456789/15032 |
identifier_str_mv |
MORAES, Juliano Oseias de. Abrasive Wear Resistance of Flexible Riser Protection Layers - Proposal of a New Test Methodology. 2005. 76 f. Dissertação (Mestrado em Engenharias) - Universidade Federal de Uberlândia, Uberlândia, 2005. |
url |
https://repositorio.ufu.br/handle/123456789/15032 |
dc.language.iso.fl_str_mv |
por |
language |
por |
dc.rights.driver.fl_str_mv |
info:eu-repo/semantics/openAccess |
eu_rights_str_mv |
openAccess |
dc.format.none.fl_str_mv |
application/pdf application/zip application/pdf application/octet-stream application/octet-stream application/octet-stream application/octet-stream |
dc.publisher.none.fl_str_mv |
Universidade Federal de Uberlândia BR Programa de Pós-graduação em Engenharia Mecânica Engenharias UFU |
publisher.none.fl_str_mv |
Universidade Federal de Uberlândia BR Programa de Pós-graduação em Engenharia Mecânica Engenharias UFU |
dc.source.none.fl_str_mv |
reponame:Repositório Institucional da UFU instname:Universidade Federal de Uberlândia (UFU) instacron:UFU |
instname_str |
Universidade Federal de Uberlândia (UFU) |
instacron_str |
UFU |
institution |
UFU |
reponame_str |
Repositório Institucional da UFU |
collection |
Repositório Institucional da UFU |
repository.name.fl_str_mv |
Repositório Institucional da UFU - Universidade Federal de Uberlândia (UFU) |
repository.mail.fl_str_mv |
diinf@dirbi.ufu.br |
_version_ |
1813711420915712000 |