Evaluation of surface changes in glass-ceramics submitted to artificial aging by simulated brushing

Detalhes bibliográficos
Autor(a) principal: Fernandes, Daniel Roberto
Data de Publicação: 2022
Outros Autores: Baeder, Fernando Martins, Silva, Daniel Furtado, Albuquerque, Ana Carolina Lyra de, Santos, Dênis Clay Lopes dos, David, Antônio Francisco, Farias, Flávio Artur Rego, Yasunaka, lson Masaru, Feltrin, Pedro Paulo, Zanetti, Raquel Virgínia
Tipo de documento: Artigo
Idioma: eng
Título da fonte: Research, Society and Development
Texto Completo: https://rsdjournal.org/index.php/rsd/article/view/31081
Resumo: The aim of this study was to evaluate the surface changes of glass ceramics, submitted to artificial aging by simulated brushing with different toothpastes, using a brushing machine designed by the authors. Twenty-four specimens were made in the form of an upper right central incisor, in color A1 and made up in color A3; divided into 4 groups with n =6. The mechanical tests were performed by a brushing machine at an ambient temperature of 37ºC, with a frequency of 250 strokes per minute, under 250mg brush pressure and simultaneous dripping of the dentifrice solution. Test times were divided into: 0; 25,000; 50,000; 75,000; 100,000; 125,000 and 150,000 strokes and the parameters analyzed by a rugosimeter. The obtained values of surface roughness (SR) were submitted to the Kolmogorov-Smirnov test (p=0.321) to verify the normality of the data distribution and, later, to the Levene test (p=0.076). The results obtained showed that the aging time did not influence the surface roughness of the glass ceramics, there were differences in surface roughness in some toothpastes. Thus, it can be concluded that the glass ceramics were susceptible to mass loss, but resistant to the action of toothpastes. Dentifrices with anti-plaque and anti-tartar characteristics can change the surface over time.
id UNIFEI_17098297a7294eaf68c276459b0d42c7
oai_identifier_str oai:ojs.pkp.sfu.ca:article/31081
network_acronym_str UNIFEI
network_name_str Research, Society and Development
repository_id_str
spelling Evaluation of surface changes in glass-ceramics submitted to artificial aging by simulated brushingEvaluación de los cambios superficiales en vitrocerámicas sometidas a envejecimiento artificial mediante cepillado simuladoAvaliação das alterações superficiais de vitrocerâmicas submetidas ao envelhecimento artificial por escovação simuladaVitrocerâmicasEscovação simuladaEnvelhecimento artificial.VitrocerámicasCepillado simuladoEnvejecimiento artificial.Glass-ceramicsSimulated brushingArtificial aging.The aim of this study was to evaluate the surface changes of glass ceramics, submitted to artificial aging by simulated brushing with different toothpastes, using a brushing machine designed by the authors. Twenty-four specimens were made in the form of an upper right central incisor, in color A1 and made up in color A3; divided into 4 groups with n =6. The mechanical tests were performed by a brushing machine at an ambient temperature of 37ºC, with a frequency of 250 strokes per minute, under 250mg brush pressure and simultaneous dripping of the dentifrice solution. Test times were divided into: 0; 25,000; 50,000; 75,000; 100,000; 125,000 and 150,000 strokes and the parameters analyzed by a rugosimeter. The obtained values of surface roughness (SR) were submitted to the Kolmogorov-Smirnov test (p=0.321) to verify the normality of the data distribution and, later, to the Levene test (p=0.076). The results obtained showed that the aging time did not influence the surface roughness of the glass ceramics, there were differences in surface roughness in some toothpastes. Thus, it can be concluded that the glass ceramics were susceptible to mass loss, but resistant to the action of toothpastes. Dentifrices with anti-plaque and anti-tartar characteristics can change the surface over time.El objetivo de este estudio fue evaluar los cambios superficiales de vitrocerámicas, sometidas a envejecimiento artificial mediante cepillado simulado con diferentes dentífricos, utilizando una máquina cepilladora diseñada por los autores. Se realizaron veinticuatro ejemplares en forma de incisivo central superior derecho, en color A1 y maquillados en color A3; divididos en 4 grupos con n =6. Las pruebas mecánicas se realizaron con una máquina cepilladora a una temperatura ambiente de 37ºC, con una frecuencia de 250 golpes por minuto, bajo una presión de cepillo de 250 mg y goteo simultáneo de la solución dentífrica. Los tiempos de prueba se dividieron en: 0; 25.000; 50.000; 75.000; 100.000; 125.000 y 150.000 golpes y los parámetros analizados por un rugosímetro. Los valores de rugosidad superficial (SR) obtenidos se sometieron a la prueba de Kolmogorov-Smirnov (p=0,321) para verificar la normalidad de la distribución de los datos y, posteriormente, a la prueba de Levene (p=0,076). Los resultados obtenidos mostraron que el tiempo de envejecimiento no influyó en la rugosidad superficial de las vitrocerámicas, existiendo diferencias en la rugosidad superficial en algunas pastas dentales. Así, se puede concluir que las vitrocerámicas fueron susceptibles a la pérdida de masa, pero resistentes a la acción de los dentífricos. Los dentífricos con características antiplaca y antisarro pueden cambiar la superficie con el tiempo.O objetivo deste estudo foi avaliar as alterações superficiais das vitrocerâmicas, submetidas ao envelhecimento artificial por escovação simulada com diferentes dentifrícios, utilizando uma máquina de escovação idealizada pelos autores. Foram confeccionados 24 corpos de prova com forma de incisivo central superior direito, na cor A1 e maquiados na cor A3; divididos em 4 grupos com n =6. Os testes mecânicos foram realizados por uma máquina de escovação à temperatura ambiente de 37ºC, com frequência de 250 golpes por minuto, sob pressão das escovas de 250mg e gotejamento simultâneo da solução de dentifrício. Os tempos de teste foram divididos em: 0; 25.000; 50.000; 75.000; 100.000; 125.000 e 150.000 golpes e os parâmetros analisados por um rugossímetro. Os valores obtidos de rugosidade superficial (RS) foram submetidos ao teste de Kolmogorov-Smirnov (p=0,321) para verificação da normalidade da distribuição dos dados e, posteriormente, ao teste de Levene (p=0,076). Os resultados obtidos mostraram que o tempo de envelhecimento não influenciou na rugosidade superficial das vitrocerâmicas, houveram diferenças de rugosidade superficialmente alguns dentifrícios. Dessa forma, pode-se concluir que as vitrocerâmicas se mostraram susceptíveis a perda de massa, mas resistentes à ação dos dentifrícios; dentifrícios com características antiplaca e antitártaro podem alterar a superfície ao longo do tempo.Research, Society and Development2022-07-03info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersionapplication/pdfhttps://rsdjournal.org/index.php/rsd/article/view/3108110.33448/rsd-v11i9.31081Research, Society and Development; Vol. 11 No. 9; e9311931081Research, Society and Development; Vol. 11 Núm. 9; e9311931081Research, Society and Development; v. 11 n. 9; e93119310812525-3409reponame:Research, Society and Developmentinstname:Universidade Federal de Itajubá (UNIFEI)instacron:UNIFEIenghttps://rsdjournal.org/index.php/rsd/article/view/31081/26937Copyright (c) 2022 Daniel Roberto Fernandes; Fernando Martins Baeder; Daniel Furtado Silva; Ana Carolina Lyra de Albuquerque; Dênis Clay Lopes dos Santos; Antônio Francisco David; Flávio Artur Rego Farias; lson Masaru Yasunaka; Pedro Paulo Feltrin; Raquel Virgínia Zanettihttps://creativecommons.org/licenses/by/4.0info:eu-repo/semantics/openAccessFernandes, Daniel RobertoBaeder, Fernando MartinsSilva, Daniel Furtado Albuquerque, Ana Carolina Lyra de Santos, Dênis Clay Lopes dosDavid, Antônio FranciscoFarias, Flávio Artur Rego Yasunaka, lson MasaruFeltrin, Pedro PauloZanetti, Raquel Virgínia2022-07-21T12:36:16Zoai:ojs.pkp.sfu.ca:article/31081Revistahttps://rsdjournal.org/index.php/rsd/indexPUBhttps://rsdjournal.org/index.php/rsd/oairsd.articles@gmail.com2525-34092525-3409opendoar:2024-01-17T09:47:34.448758Research, Society and Development - Universidade Federal de Itajubá (UNIFEI)false
dc.title.none.fl_str_mv Evaluation of surface changes in glass-ceramics submitted to artificial aging by simulated brushing
Evaluación de los cambios superficiales en vitrocerámicas sometidas a envejecimiento artificial mediante cepillado simulado
Avaliação das alterações superficiais de vitrocerâmicas submetidas ao envelhecimento artificial por escovação simulada
title Evaluation of surface changes in glass-ceramics submitted to artificial aging by simulated brushing
spellingShingle Evaluation of surface changes in glass-ceramics submitted to artificial aging by simulated brushing
Fernandes, Daniel Roberto
Vitrocerâmicas
Escovação simulada
Envelhecimento artificial.
Vitrocerámicas
Cepillado simulado
Envejecimiento artificial.
Glass-ceramics
Simulated brushing
Artificial aging.
title_short Evaluation of surface changes in glass-ceramics submitted to artificial aging by simulated brushing
title_full Evaluation of surface changes in glass-ceramics submitted to artificial aging by simulated brushing
title_fullStr Evaluation of surface changes in glass-ceramics submitted to artificial aging by simulated brushing
title_full_unstemmed Evaluation of surface changes in glass-ceramics submitted to artificial aging by simulated brushing
title_sort Evaluation of surface changes in glass-ceramics submitted to artificial aging by simulated brushing
author Fernandes, Daniel Roberto
author_facet Fernandes, Daniel Roberto
Baeder, Fernando Martins
Silva, Daniel Furtado
Albuquerque, Ana Carolina Lyra de
Santos, Dênis Clay Lopes dos
David, Antônio Francisco
Farias, Flávio Artur Rego
Yasunaka, lson Masaru
Feltrin, Pedro Paulo
Zanetti, Raquel Virgínia
author_role author
author2 Baeder, Fernando Martins
Silva, Daniel Furtado
Albuquerque, Ana Carolina Lyra de
Santos, Dênis Clay Lopes dos
David, Antônio Francisco
Farias, Flávio Artur Rego
Yasunaka, lson Masaru
Feltrin, Pedro Paulo
Zanetti, Raquel Virgínia
author2_role author
author
author
author
author
author
author
author
author
dc.contributor.author.fl_str_mv Fernandes, Daniel Roberto
Baeder, Fernando Martins
Silva, Daniel Furtado
Albuquerque, Ana Carolina Lyra de
Santos, Dênis Clay Lopes dos
David, Antônio Francisco
Farias, Flávio Artur Rego
Yasunaka, lson Masaru
Feltrin, Pedro Paulo
Zanetti, Raquel Virgínia
dc.subject.por.fl_str_mv Vitrocerâmicas
Escovação simulada
Envelhecimento artificial.
Vitrocerámicas
Cepillado simulado
Envejecimiento artificial.
Glass-ceramics
Simulated brushing
Artificial aging.
topic Vitrocerâmicas
Escovação simulada
Envelhecimento artificial.
Vitrocerámicas
Cepillado simulado
Envejecimiento artificial.
Glass-ceramics
Simulated brushing
Artificial aging.
description The aim of this study was to evaluate the surface changes of glass ceramics, submitted to artificial aging by simulated brushing with different toothpastes, using a brushing machine designed by the authors. Twenty-four specimens were made in the form of an upper right central incisor, in color A1 and made up in color A3; divided into 4 groups with n =6. The mechanical tests were performed by a brushing machine at an ambient temperature of 37ºC, with a frequency of 250 strokes per minute, under 250mg brush pressure and simultaneous dripping of the dentifrice solution. Test times were divided into: 0; 25,000; 50,000; 75,000; 100,000; 125,000 and 150,000 strokes and the parameters analyzed by a rugosimeter. The obtained values of surface roughness (SR) were submitted to the Kolmogorov-Smirnov test (p=0.321) to verify the normality of the data distribution and, later, to the Levene test (p=0.076). The results obtained showed that the aging time did not influence the surface roughness of the glass ceramics, there were differences in surface roughness in some toothpastes. Thus, it can be concluded that the glass ceramics were susceptible to mass loss, but resistant to the action of toothpastes. Dentifrices with anti-plaque and anti-tartar characteristics can change the surface over time.
publishDate 2022
dc.date.none.fl_str_mv 2022-07-03
dc.type.driver.fl_str_mv info:eu-repo/semantics/article
info:eu-repo/semantics/publishedVersion
format article
status_str publishedVersion
dc.identifier.uri.fl_str_mv https://rsdjournal.org/index.php/rsd/article/view/31081
10.33448/rsd-v11i9.31081
url https://rsdjournal.org/index.php/rsd/article/view/31081
identifier_str_mv 10.33448/rsd-v11i9.31081
dc.language.iso.fl_str_mv eng
language eng
dc.relation.none.fl_str_mv https://rsdjournal.org/index.php/rsd/article/view/31081/26937
dc.rights.driver.fl_str_mv https://creativecommons.org/licenses/by/4.0
info:eu-repo/semantics/openAccess
rights_invalid_str_mv https://creativecommons.org/licenses/by/4.0
eu_rights_str_mv openAccess
dc.format.none.fl_str_mv application/pdf
dc.publisher.none.fl_str_mv Research, Society and Development
publisher.none.fl_str_mv Research, Society and Development
dc.source.none.fl_str_mv Research, Society and Development; Vol. 11 No. 9; e9311931081
Research, Society and Development; Vol. 11 Núm. 9; e9311931081
Research, Society and Development; v. 11 n. 9; e9311931081
2525-3409
reponame:Research, Society and Development
instname:Universidade Federal de Itajubá (UNIFEI)
instacron:UNIFEI
instname_str Universidade Federal de Itajubá (UNIFEI)
instacron_str UNIFEI
institution UNIFEI
reponame_str Research, Society and Development
collection Research, Society and Development
repository.name.fl_str_mv Research, Society and Development - Universidade Federal de Itajubá (UNIFEI)
repository.mail.fl_str_mv rsd.articles@gmail.com
_version_ 1797052715506860032