Abrasive wear of two glass ionomer cements after simulated toothbrushing

Detalhes bibliográficos
Autor(a) principal: Freitas, Márcia Furtado Antunes de
Data de Publicação: 2011
Outros Autores: Imai, Leandro Jum, Freitas, César Antunes de, Bianchi, Eduardo Carlos [UNESP], Almeida, Carina Thaís de, Martins Filho, Ismar Eduardo
Tipo de documento: Artigo
Idioma: eng
Título da fonte: Repositório Institucional da UNESP
Texto Completo: http://www.univille.edu.br/pt-BR/departamentos/odontologia/revista-rsbo/edicoes--2011/RSBO---v8---n03/725748
http://hdl.handle.net/11449/134691
Resumo: Introduction and objective: Glass ionomer cement, which was first introduced in Dentistry in 1972, presents good qualities such as aesthetics, fluoride release and adhesion to dental tissues. Because of its preventive characteristics regarding to dental caries, glass ionomer cement has been used for Atraumatic Restorative Treatment (ART), as reported by Frencken and Holmgren [6], meeting the principles announced by the World Health Organization (WHO) for application to large population groups without regular access to dental care. Material and methods: In this present study, the abrasive wear strength of two glass-ionomer cements (Vidrion R® and ChemFlex®) was evaluated through toothbrushing machine. Classic® toothbrushes with soft bristles and Sorriso® dentifrice were also used for the study. Results: Student-t test showed significant difference between both groups, with tobs value = 9.4411 at p < 0.05. Conclusion: It can be concluded that the wear rate caused by toothbrush/dentifrice was higher for Vidrion R® (52.00 mg) than ChemFlex® (5.57 mg).
id UNSP_39945dd04d076f131bc6780c5b13c687
oai_identifier_str oai:repositorio.unesp.br:11449/134691
network_acronym_str UNSP
network_name_str Repositório Institucional da UNESP
repository_id_str 2946
spelling Abrasive wear of two glass ionomer cements after simulated toothbrushingIntroduction and objective: Glass ionomer cement, which was first introduced in Dentistry in 1972, presents good qualities such as aesthetics, fluoride release and adhesion to dental tissues. Because of its preventive characteristics regarding to dental caries, glass ionomer cement has been used for Atraumatic Restorative Treatment (ART), as reported by Frencken and Holmgren [6], meeting the principles announced by the World Health Organization (WHO) for application to large population groups without regular access to dental care. Material and methods: In this present study, the abrasive wear strength of two glass-ionomer cements (Vidrion R® and ChemFlex®) was evaluated through toothbrushing machine. Classic® toothbrushes with soft bristles and Sorriso® dentifrice were also used for the study. Results: Student-t test showed significant difference between both groups, with tobs value = 9.4411 at p < 0.05. Conclusion: It can be concluded that the wear rate caused by toothbrush/dentifrice was higher for Vidrion R® (52.00 mg) than ChemFlex® (5.57 mg).Universidade Estadual Paulista Júlio de Mesquita Filho, Departamento de Engenharia Mecânica, Faculdade de Engenharia de Bauru, Bauru, Av. Luiz Edmundo Carrijo Coube, 14-01 - Laboratório de Usinagem por Abrasão - FEB - DEM, Vargem Limpa, CEP 17033360, SP, BrasilDepartment of Pediatric Dentistry, Orthodontics and Community Dentistry, Bauru Dental School, University of Sao Paulo – Bauru – Sao Paulo – Brazil.Department of Operative Dentistry, Endodontics and Dental Materials, Bauru Dental School, University of Sao Paulo – Bauru – Sao Paulo – Brazil.Universidade Estadual Paulista Júlio de Mesquita Filho, Departamento de Engenharia Mecânica, Faculdade de Engenharia de Bauru, Bauru, Av. Luiz Edmundo Carrijo Coube, 14-01 - Laboratório de Usinagem por Abrasão - FEB - DEM, Vargem Limpa, CEP 17033360, SP, BrasilUniversidade Estadual Paulista (Unesp)Universidade de São Paulo (USP)Freitas, Márcia Furtado Antunes deImai, Leandro JumFreitas, César Antunes deBianchi, Eduardo Carlos [UNESP]Almeida, Carina Thaís deMartins Filho, Ismar Eduardo2016-03-02T12:57:59Z2016-03-02T12:57:59Z2011info:eu-repo/semantics/publishedVersioninfo:eu-repo/semantics/article287-293application/pdfhttp://www.univille.edu.br/pt-BR/departamentos/odontologia/revista-rsbo/edicoes--2011/RSBO---v8---n03/725748RSBO. Revista Sul-Brasileira de Odontologia, v. 8, n. 3, p. 287-293, 2011.1806-7727http://hdl.handle.net/11449/134691ISSN1806-7727-2011-08-03-287-293.pdf8188237078123345347799711823886185145598358412951099152007574921Currículo Lattesreponame:Repositório Institucional da UNESPinstname:Universidade Estadual Paulista (UNESP)instacron:UNESPengRSBO. Revista Sul-Brasileira de Odontologiainfo:eu-repo/semantics/openAccess2024-06-28T13:54:38Zoai:repositorio.unesp.br:11449/134691Repositório InstitucionalPUBhttp://repositorio.unesp.br/oai/requestopendoar:29462024-08-05T16:12:03.035498Repositório Institucional da UNESP - Universidade Estadual Paulista (UNESP)false
dc.title.none.fl_str_mv Abrasive wear of two glass ionomer cements after simulated toothbrushing
title Abrasive wear of two glass ionomer cements after simulated toothbrushing
spellingShingle Abrasive wear of two glass ionomer cements after simulated toothbrushing
Freitas, Márcia Furtado Antunes de
title_short Abrasive wear of two glass ionomer cements after simulated toothbrushing
title_full Abrasive wear of two glass ionomer cements after simulated toothbrushing
title_fullStr Abrasive wear of two glass ionomer cements after simulated toothbrushing
title_full_unstemmed Abrasive wear of two glass ionomer cements after simulated toothbrushing
title_sort Abrasive wear of two glass ionomer cements after simulated toothbrushing
author Freitas, Márcia Furtado Antunes de
author_facet Freitas, Márcia Furtado Antunes de
Imai, Leandro Jum
Freitas, César Antunes de
Bianchi, Eduardo Carlos [UNESP]
Almeida, Carina Thaís de
Martins Filho, Ismar Eduardo
author_role author
author2 Imai, Leandro Jum
Freitas, César Antunes de
Bianchi, Eduardo Carlos [UNESP]
Almeida, Carina Thaís de
Martins Filho, Ismar Eduardo
author2_role author
author
author
author
author
dc.contributor.none.fl_str_mv Universidade Estadual Paulista (Unesp)
Universidade de São Paulo (USP)
dc.contributor.author.fl_str_mv Freitas, Márcia Furtado Antunes de
Imai, Leandro Jum
Freitas, César Antunes de
Bianchi, Eduardo Carlos [UNESP]
Almeida, Carina Thaís de
Martins Filho, Ismar Eduardo
description Introduction and objective: Glass ionomer cement, which was first introduced in Dentistry in 1972, presents good qualities such as aesthetics, fluoride release and adhesion to dental tissues. Because of its preventive characteristics regarding to dental caries, glass ionomer cement has been used for Atraumatic Restorative Treatment (ART), as reported by Frencken and Holmgren [6], meeting the principles announced by the World Health Organization (WHO) for application to large population groups without regular access to dental care. Material and methods: In this present study, the abrasive wear strength of two glass-ionomer cements (Vidrion R® and ChemFlex®) was evaluated through toothbrushing machine. Classic® toothbrushes with soft bristles and Sorriso® dentifrice were also used for the study. Results: Student-t test showed significant difference between both groups, with tobs value = 9.4411 at p < 0.05. Conclusion: It can be concluded that the wear rate caused by toothbrush/dentifrice was higher for Vidrion R® (52.00 mg) than ChemFlex® (5.57 mg).
publishDate 2011
dc.date.none.fl_str_mv 2011
2016-03-02T12:57:59Z
2016-03-02T12:57:59Z
dc.type.status.fl_str_mv info:eu-repo/semantics/publishedVersion
dc.type.driver.fl_str_mv info:eu-repo/semantics/article
format article
status_str publishedVersion
dc.identifier.uri.fl_str_mv http://www.univille.edu.br/pt-BR/departamentos/odontologia/revista-rsbo/edicoes--2011/RSBO---v8---n03/725748
RSBO. Revista Sul-Brasileira de Odontologia, v. 8, n. 3, p. 287-293, 2011.
1806-7727
http://hdl.handle.net/11449/134691
ISSN1806-7727-2011-08-03-287-293.pdf
8188237078123345
3477997118238861
8514559835841295
1099152007574921
url http://www.univille.edu.br/pt-BR/departamentos/odontologia/revista-rsbo/edicoes--2011/RSBO---v8---n03/725748
http://hdl.handle.net/11449/134691
identifier_str_mv RSBO. Revista Sul-Brasileira de Odontologia, v. 8, n. 3, p. 287-293, 2011.
1806-7727
ISSN1806-7727-2011-08-03-287-293.pdf
8188237078123345
3477997118238861
8514559835841295
1099152007574921
dc.language.iso.fl_str_mv eng
language eng
dc.relation.none.fl_str_mv RSBO. Revista Sul-Brasileira de Odontologia
dc.rights.driver.fl_str_mv info:eu-repo/semantics/openAccess
eu_rights_str_mv openAccess
dc.format.none.fl_str_mv 287-293
application/pdf
dc.source.none.fl_str_mv Currículo Lattes
reponame:Repositório Institucional da UNESP
instname:Universidade Estadual Paulista (UNESP)
instacron:UNESP
instname_str Universidade Estadual Paulista (UNESP)
instacron_str UNESP
institution UNESP
reponame_str Repositório Institucional da UNESP
collection Repositório Institucional da UNESP
repository.name.fl_str_mv Repositório Institucional da UNESP - Universidade Estadual Paulista (UNESP)
repository.mail.fl_str_mv
_version_ 1808128617304031232