Degree of conversion and molecular weight of one denture base and three reline resins submitted post-polymerization treatments

Detalhes bibliográficos
Autor(a) principal: Urban, Vanessa Migliorini [UNESP]
Data de Publicação: 2007
Outros Autores: Machado, Ana Lucia [UNESP], Vergani, Carlos Eduardo [UNESP], Jorge, Érica Gouveia [UNESP], dos Santos, Luís Presley Serejo, Leite, Edson Roberto, Canevarolo, Sebastião Vicente
Tipo de documento: Artigo
Idioma: eng
Título da fonte: Repositório Institucional da UNESP
Texto Completo: http://dx.doi.org/10.1590/S1516-14392007000200016
http://hdl.handle.net/11449/69604
Resumo: The effect of post-polymerization treatments (MW-microwave irradiatron and WB-water-bath) on the degree of conversion (DC) of three reline resins (Ufi Gel hard-U, Kooliner-K, and Tokuso Rebase Fast-T) and one denture base resin (Lucitone 550-L), submitted to two polymerization cycles (LS-short and LL-long), was evaluated by using FT-Raman spectroscopy (n = 5). The molecular weight (Mw) of the powder of all materials and of K polymerized specimens (control; MW; and WB; n = 3) was analyzed using GPC. DC data were analyzed using Kruskal-Wallis test (α = .05). For control specimens, there were no significant differences between U (68%) and LL (77%) and among LL, K (81%), and T (84%). LS (92%) had the highest DC (P<0.05). Only material K exhibited an increased DC after WB (P<0.05). All powders had Mw from 4.0 × 105 to 6.5 × 105 and narrow Mw distributions (2.1 to 3.6). Polymerization and post-polymerization produced K specimens with Mw similar to that of K powder.
id UNSP_6ce3aa0615db60c12bb106e43bf4f1c2
oai_identifier_str oai:repositorio.unesp.br:11449/69604
network_acronym_str UNSP
network_name_str Repositório Institucional da UNESP
repository_id_str 2946
spelling Degree of conversion and molecular weight of one denture base and three reline resins submitted post-polymerization treatmentsDegree of conversionMolecular weightPost-polymerization treatmentReline resinMicrowave irradiationPolymerizationResinsKruskal-Wallis testReline resinsDental prosthesesThe effect of post-polymerization treatments (MW-microwave irradiatron and WB-water-bath) on the degree of conversion (DC) of three reline resins (Ufi Gel hard-U, Kooliner-K, and Tokuso Rebase Fast-T) and one denture base resin (Lucitone 550-L), submitted to two polymerization cycles (LS-short and LL-long), was evaluated by using FT-Raman spectroscopy (n = 5). The molecular weight (Mw) of the powder of all materials and of K polymerized specimens (control; MW; and WB; n = 3) was analyzed using GPC. DC data were analyzed using Kruskal-Wallis test (α = .05). For control specimens, there were no significant differences between U (68%) and LL (77%) and among LL, K (81%), and T (84%). LS (92%) had the highest DC (P<0.05). Only material K exhibited an increased DC after WB (P<0.05). All powders had Mw from 4.0 × 105 to 6.5 × 105 and narrow Mw distributions (2.1 to 3.6). Polymerization and post-polymerization produced K specimens with Mw similar to that of K powder.Department of Dental Materials and Prosthodontics Araraquara Dental School São Paulo State University, Rua Humaitá, 1680, 14801-903 Araraquara, SPInterdisciplinary Laboratory of Eletrochemistry and Ceramics Department of Chemistry São Carlos Federal University, Rodovia Washington Luis (SP - 310), 13565-905 São Carlos, SPDepartment of Material Engineering São Carlos Federal University, Rodovia Washington Luis (SP - 310), 13565-905 São Carlos, SPDepartment of Dental Materials and Prosthodontics Araraquara Dental School São Paulo State University, Rua Humaitá, 1680, 14801-903 Araraquara, SPUniversidade Estadual Paulista (Unesp)Universidade Federal de São Carlos (UFSCar)Urban, Vanessa Migliorini [UNESP]Machado, Ana Lucia [UNESP]Vergani, Carlos Eduardo [UNESP]Jorge, Érica Gouveia [UNESP]dos Santos, Luís Presley SerejoLeite, Edson RobertoCanevarolo, Sebastião Vicente2014-05-27T11:22:26Z2014-05-27T11:22:26Z2007-04-01info:eu-repo/semantics/publishedVersioninfo:eu-repo/semantics/article191-197application/pdfhttp://dx.doi.org/10.1590/S1516-14392007000200016Materials Research, v. 10, n. 2, p. 191-197, 2007.1516-1439http://hdl.handle.net/11449/6960410.1590/S1516-14392007000200016S1516-143920070002000162-s2.0-351488751332-s2.0-35148875133.pdf800024878184258730031305224278200000-0002-7375-4714Scopusreponame:Repositório Institucional da UNESPinstname:Universidade Estadual Paulista (UNESP)instacron:UNESPengMaterials Research1.1030,398info:eu-repo/semantics/openAccess2024-09-27T14:57:18Zoai:repositorio.unesp.br:11449/69604Repositório InstitucionalPUBhttp://repositorio.unesp.br/oai/requestrepositoriounesp@unesp.bropendoar:29462024-09-27T14:57:18Repositório Institucional da UNESP - Universidade Estadual Paulista (UNESP)false
dc.title.none.fl_str_mv Degree of conversion and molecular weight of one denture base and three reline resins submitted post-polymerization treatments
title Degree of conversion and molecular weight of one denture base and three reline resins submitted post-polymerization treatments
spellingShingle Degree of conversion and molecular weight of one denture base and three reline resins submitted post-polymerization treatments
Urban, Vanessa Migliorini [UNESP]
Degree of conversion
Molecular weight
Post-polymerization treatment
Reline resin
Microwave irradiation
Polymerization
Resins
Kruskal-Wallis test
Reline resins
Dental prostheses
title_short Degree of conversion and molecular weight of one denture base and three reline resins submitted post-polymerization treatments
title_full Degree of conversion and molecular weight of one denture base and three reline resins submitted post-polymerization treatments
title_fullStr Degree of conversion and molecular weight of one denture base and three reline resins submitted post-polymerization treatments
title_full_unstemmed Degree of conversion and molecular weight of one denture base and three reline resins submitted post-polymerization treatments
title_sort Degree of conversion and molecular weight of one denture base and three reline resins submitted post-polymerization treatments
author Urban, Vanessa Migliorini [UNESP]
author_facet Urban, Vanessa Migliorini [UNESP]
Machado, Ana Lucia [UNESP]
Vergani, Carlos Eduardo [UNESP]
Jorge, Érica Gouveia [UNESP]
dos Santos, Luís Presley Serejo
Leite, Edson Roberto
Canevarolo, Sebastião Vicente
author_role author
author2 Machado, Ana Lucia [UNESP]
Vergani, Carlos Eduardo [UNESP]
Jorge, Érica Gouveia [UNESP]
dos Santos, Luís Presley Serejo
Leite, Edson Roberto
Canevarolo, Sebastião Vicente
author2_role author
author
author
author
author
author
dc.contributor.none.fl_str_mv Universidade Estadual Paulista (Unesp)
Universidade Federal de São Carlos (UFSCar)
dc.contributor.author.fl_str_mv Urban, Vanessa Migliorini [UNESP]
Machado, Ana Lucia [UNESP]
Vergani, Carlos Eduardo [UNESP]
Jorge, Érica Gouveia [UNESP]
dos Santos, Luís Presley Serejo
Leite, Edson Roberto
Canevarolo, Sebastião Vicente
dc.subject.por.fl_str_mv Degree of conversion
Molecular weight
Post-polymerization treatment
Reline resin
Microwave irradiation
Polymerization
Resins
Kruskal-Wallis test
Reline resins
Dental prostheses
topic Degree of conversion
Molecular weight
Post-polymerization treatment
Reline resin
Microwave irradiation
Polymerization
Resins
Kruskal-Wallis test
Reline resins
Dental prostheses
description The effect of post-polymerization treatments (MW-microwave irradiatron and WB-water-bath) on the degree of conversion (DC) of three reline resins (Ufi Gel hard-U, Kooliner-K, and Tokuso Rebase Fast-T) and one denture base resin (Lucitone 550-L), submitted to two polymerization cycles (LS-short and LL-long), was evaluated by using FT-Raman spectroscopy (n = 5). The molecular weight (Mw) of the powder of all materials and of K polymerized specimens (control; MW; and WB; n = 3) was analyzed using GPC. DC data were analyzed using Kruskal-Wallis test (α = .05). For control specimens, there were no significant differences between U (68%) and LL (77%) and among LL, K (81%), and T (84%). LS (92%) had the highest DC (P<0.05). Only material K exhibited an increased DC after WB (P<0.05). All powders had Mw from 4.0 × 105 to 6.5 × 105 and narrow Mw distributions (2.1 to 3.6). Polymerization and post-polymerization produced K specimens with Mw similar to that of K powder.
publishDate 2007
dc.date.none.fl_str_mv 2007-04-01
2014-05-27T11:22:26Z
2014-05-27T11:22:26Z
dc.type.status.fl_str_mv info:eu-repo/semantics/publishedVersion
dc.type.driver.fl_str_mv info:eu-repo/semantics/article
format article
status_str publishedVersion
dc.identifier.uri.fl_str_mv http://dx.doi.org/10.1590/S1516-14392007000200016
Materials Research, v. 10, n. 2, p. 191-197, 2007.
1516-1439
http://hdl.handle.net/11449/69604
10.1590/S1516-14392007000200016
S1516-14392007000200016
2-s2.0-35148875133
2-s2.0-35148875133.pdf
8000248781842587
3003130522427820
0000-0002-7375-4714
url http://dx.doi.org/10.1590/S1516-14392007000200016
http://hdl.handle.net/11449/69604
identifier_str_mv Materials Research, v. 10, n. 2, p. 191-197, 2007.
1516-1439
10.1590/S1516-14392007000200016
S1516-14392007000200016
2-s2.0-35148875133
2-s2.0-35148875133.pdf
8000248781842587
3003130522427820
0000-0002-7375-4714
dc.language.iso.fl_str_mv eng
language eng
dc.relation.none.fl_str_mv Materials Research
1.103
0,398
dc.rights.driver.fl_str_mv info:eu-repo/semantics/openAccess
eu_rights_str_mv openAccess
dc.format.none.fl_str_mv 191-197
application/pdf
dc.source.none.fl_str_mv Scopus
reponame:Repositório Institucional da UNESP
instname:Universidade Estadual Paulista (UNESP)
instacron:UNESP
instname_str Universidade Estadual Paulista (UNESP)
instacron_str UNESP
institution UNESP
reponame_str Repositório Institucional da UNESP
collection Repositório Institucional da UNESP
repository.name.fl_str_mv Repositório Institucional da UNESP - Universidade Estadual Paulista (UNESP)
repository.mail.fl_str_mv repositoriounesp@unesp.br
_version_ 1813546497804861440