New compositions of fluoroindate glasses with higher chemical resistance
Autor(a) principal: | |
---|---|
Data de Publicação: | 1998 |
Outros Autores: | , |
Tipo de documento: | Artigo |
Idioma: | eng |
Título da fonte: | Química Nova (Online) |
Texto Completo: | http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40421998000300025 |
Resumo: | In this paper, glasses in the systems In-Ba-Mg and In-Ba-Zn-Sr-Mg were water leachead at 80ºC showing surface degradation after 72 hours of leaching. The extent of such degradation is determined by the solubility and the concentration of the elemental fluorides that constitute the glasses. The formation of a layer of crystallized phases on the surface of the samples was observed. Small weight losses were registered and the absence of water on the glass matrix after the attack suggested that the use of MgF2 in the systems studied can lead to better results against moisture corrosion when compared to other fluoride glasses such as the fluorozirconates. |
id |
SBQ-3_58021d913b10fefe2d03347a23949f3b |
---|---|
oai_identifier_str |
oai:scielo:S0100-40421998000300025 |
network_acronym_str |
SBQ-3 |
network_name_str |
Química Nova (Online) |
repository_id_str |
|
spelling |
New compositions of fluoroindate glasses with higher chemical resistanceglassfluoroindatewaterresistanceIn this paper, glasses in the systems In-Ba-Mg and In-Ba-Zn-Sr-Mg were water leachead at 80ºC showing surface degradation after 72 hours of leaching. The extent of such degradation is determined by the solubility and the concentration of the elemental fluorides that constitute the glasses. The formation of a layer of crystallized phases on the surface of the samples was observed. Small weight losses were registered and the absence of water on the glass matrix after the attack suggested that the use of MgF2 in the systems studied can lead to better results against moisture corrosion when compared to other fluoride glasses such as the fluorozirconates.Sociedade Brasileira de Química1998-06-01info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersiontext/htmlhttp://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40421998000300025Química Nova v.21 n.3 1998reponame:Química Nova (Online)instname:Sociedade Brasileira de Química (SBQ)instacron:SBQ10.1590/S0100-40421998000300025info:eu-repo/semantics/openAccessCosta,B. J.Soufiane,A.Messaddeq,Y.eng2003-12-04T00:00:00Zoai:scielo:S0100-40421998000300025Revistahttps://www.scielo.br/j/qn/ONGhttps://old.scielo.br/oai/scielo-oai.phpquimicanova@sbq.org.br1678-70640100-4042opendoar:2003-12-04T00:00Química Nova (Online) - Sociedade Brasileira de Química (SBQ)false |
dc.title.none.fl_str_mv |
New compositions of fluoroindate glasses with higher chemical resistance |
title |
New compositions of fluoroindate glasses with higher chemical resistance |
spellingShingle |
New compositions of fluoroindate glasses with higher chemical resistance Costa,B. J. glass fluoroindate water resistance |
title_short |
New compositions of fluoroindate glasses with higher chemical resistance |
title_full |
New compositions of fluoroindate glasses with higher chemical resistance |
title_fullStr |
New compositions of fluoroindate glasses with higher chemical resistance |
title_full_unstemmed |
New compositions of fluoroindate glasses with higher chemical resistance |
title_sort |
New compositions of fluoroindate glasses with higher chemical resistance |
author |
Costa,B. J. |
author_facet |
Costa,B. J. Soufiane,A. Messaddeq,Y. |
author_role |
author |
author2 |
Soufiane,A. Messaddeq,Y. |
author2_role |
author author |
dc.contributor.author.fl_str_mv |
Costa,B. J. Soufiane,A. Messaddeq,Y. |
dc.subject.por.fl_str_mv |
glass fluoroindate water resistance |
topic |
glass fluoroindate water resistance |
description |
In this paper, glasses in the systems In-Ba-Mg and In-Ba-Zn-Sr-Mg were water leachead at 80ºC showing surface degradation after 72 hours of leaching. The extent of such degradation is determined by the solubility and the concentration of the elemental fluorides that constitute the glasses. The formation of a layer of crystallized phases on the surface of the samples was observed. Small weight losses were registered and the absence of water on the glass matrix after the attack suggested that the use of MgF2 in the systems studied can lead to better results against moisture corrosion when compared to other fluoride glasses such as the fluorozirconates. |
publishDate |
1998 |
dc.date.none.fl_str_mv |
1998-06-01 |
dc.type.driver.fl_str_mv |
info:eu-repo/semantics/article |
dc.type.status.fl_str_mv |
info:eu-repo/semantics/publishedVersion |
format |
article |
status_str |
publishedVersion |
dc.identifier.uri.fl_str_mv |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40421998000300025 |
url |
http://old.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40421998000300025 |
dc.language.iso.fl_str_mv |
eng |
language |
eng |
dc.relation.none.fl_str_mv |
10.1590/S0100-40421998000300025 |
dc.rights.driver.fl_str_mv |
info:eu-repo/semantics/openAccess |
eu_rights_str_mv |
openAccess |
dc.format.none.fl_str_mv |
text/html |
dc.publisher.none.fl_str_mv |
Sociedade Brasileira de Química |
publisher.none.fl_str_mv |
Sociedade Brasileira de Química |
dc.source.none.fl_str_mv |
Química Nova v.21 n.3 1998 reponame:Química Nova (Online) instname:Sociedade Brasileira de Química (SBQ) instacron:SBQ |
instname_str |
Sociedade Brasileira de Química (SBQ) |
instacron_str |
SBQ |
institution |
SBQ |
reponame_str |
Química Nova (Online) |
collection |
Química Nova (Online) |
repository.name.fl_str_mv |
Química Nova (Online) - Sociedade Brasileira de Química (SBQ) |
repository.mail.fl_str_mv |
quimicanova@sbq.org.br |
_version_ |
1750318100502282240 |