New compositions of fluoroindate glasses with higher chemical resistance
Autor(a) principal: | |
---|---|
Data de Publicação: | 1998 |
Outros Autores: | , |
Tipo de documento: | Artigo |
Idioma: | eng |
Título da fonte: | Repositório Institucional da UNESP |
Texto Completo: | http://dx.doi.org/10.1590/S0100-40421998000300025 http://hdl.handle.net/11449/27558 |
Resumo: | In this paper, glasses in the systems In-Ba-Mg and In-Ba-Zn-Sr-Mg were water leachead at 80ºC showing surface degradation after 72 hours of leaching. The extent of such degradation is determined by the solubility and the concentration of the elemental fluorides that constitute the glasses. The formation of a layer of crystallized phases on the surface of the samples was observed. Small weight losses were registered and the absence of water on the glass matrix after the attack suggested that the use of MgF2 in the systems studied can lead to better results against moisture corrosion when compared to other fluoride glasses such as the fluorozirconates. |
id |
UNSP_355ffcc31544b0846b62574627525eba |
---|---|
oai_identifier_str |
oai:repositorio.unesp.br:11449/27558 |
network_acronym_str |
UNSP |
network_name_str |
Repositório Institucional da UNESP |
repository_id_str |
2946 |
spelling |
New compositions of fluoroindate glasses with higher chemical resistanceThe chemical resistance of fluoride glasses in aqueous solution is a very important factor oncerning the technological applications of these materialsglassfluoroindatewaterresistanceIn this paper, glasses in the systems In-Ba-Mg and In-Ba-Zn-Sr-Mg were water leachead at 80ºC showing surface degradation after 72 hours of leaching. The extent of such degradation is determined by the solubility and the concentration of the elemental fluorides that constitute the glasses. The formation of a layer of crystallized phases on the surface of the samples was observed. Small weight losses were registered and the absence of water on the glass matrix after the attack suggested that the use of MgF2 in the systems studied can lead to better results against moisture corrosion when compared to other fluoride glasses such as the fluorozirconates.USP IFSCFull Spectrum, Inc.UNESP IQUNESP IQSociedade Brasileira de QuímicaUniversidade de São Paulo (USP)Full Spectrum, Inc.Universidade Estadual Paulista (Unesp)Costa, B. J.Soufiane, A.Messaddeq, Younes [UNESP]2014-05-20T15:10:16Z2014-05-20T15:10:16Z1998-06-01info:eu-repo/semantics/publishedVersioninfo:eu-repo/semantics/article370-371application/pdfhttp://dx.doi.org/10.1590/S0100-40421998000300025Química Nova. Sociedade Brasileira de Química, v. 21, n. 3, p. 370-371, 1998.0100-4042http://hdl.handle.net/11449/2755810.1590/S0100-40421998000300025S0100-40421998000300025S0100-40421998000300025.pdf2998503841917815SciELOreponame:Repositório Institucional da UNESPinstname:Universidade Estadual Paulista (UNESP)instacron:UNESPengQuímica Nova0.6460,255info:eu-repo/semantics/openAccess2023-12-18T06:12:51Zoai:repositorio.unesp.br:11449/27558Repositório InstitucionalPUBhttp://repositorio.unesp.br/oai/requestopendoar:29462024-08-05T20:36:46.879351Repositório Institucional da UNESP - Universidade Estadual Paulista (UNESP)false |
dc.title.none.fl_str_mv |
New compositions of fluoroindate glasses with higher chemical resistance The chemical resistance of fluoride glasses in aqueous solution is a very important factor oncerning the technological applications of these materials |
title |
New compositions of fluoroindate glasses with higher chemical resistance |
spellingShingle |
New compositions of fluoroindate glasses with higher chemical resistance Costa, B. J. glass fluoroindate water resistance |
title_short |
New compositions of fluoroindate glasses with higher chemical resistance |
title_full |
New compositions of fluoroindate glasses with higher chemical resistance |
title_fullStr |
New compositions of fluoroindate glasses with higher chemical resistance |
title_full_unstemmed |
New compositions of fluoroindate glasses with higher chemical resistance |
title_sort |
New compositions of fluoroindate glasses with higher chemical resistance |
author |
Costa, B. J. |
author_facet |
Costa, B. J. Soufiane, A. Messaddeq, Younes [UNESP] |
author_role |
author |
author2 |
Soufiane, A. Messaddeq, Younes [UNESP] |
author2_role |
author author |
dc.contributor.none.fl_str_mv |
Universidade de São Paulo (USP) Full Spectrum, Inc. Universidade Estadual Paulista (Unesp) |
dc.contributor.author.fl_str_mv |
Costa, B. J. Soufiane, A. Messaddeq, Younes [UNESP] |
dc.subject.por.fl_str_mv |
glass fluoroindate water resistance |
topic |
glass fluoroindate water resistance |
description |
In this paper, glasses in the systems In-Ba-Mg and In-Ba-Zn-Sr-Mg were water leachead at 80ºC showing surface degradation after 72 hours of leaching. The extent of such degradation is determined by the solubility and the concentration of the elemental fluorides that constitute the glasses. The formation of a layer of crystallized phases on the surface of the samples was observed. Small weight losses were registered and the absence of water on the glass matrix after the attack suggested that the use of MgF2 in the systems studied can lead to better results against moisture corrosion when compared to other fluoride glasses such as the fluorozirconates. |
publishDate |
1998 |
dc.date.none.fl_str_mv |
1998-06-01 2014-05-20T15:10:16Z 2014-05-20T15:10:16Z |
dc.type.status.fl_str_mv |
info:eu-repo/semantics/publishedVersion |
dc.type.driver.fl_str_mv |
info:eu-repo/semantics/article |
format |
article |
status_str |
publishedVersion |
dc.identifier.uri.fl_str_mv |
http://dx.doi.org/10.1590/S0100-40421998000300025 Química Nova. Sociedade Brasileira de Química, v. 21, n. 3, p. 370-371, 1998. 0100-4042 http://hdl.handle.net/11449/27558 10.1590/S0100-40421998000300025 S0100-40421998000300025 S0100-40421998000300025.pdf 2998503841917815 |
url |
http://dx.doi.org/10.1590/S0100-40421998000300025 http://hdl.handle.net/11449/27558 |
identifier_str_mv |
Química Nova. Sociedade Brasileira de Química, v. 21, n. 3, p. 370-371, 1998. 0100-4042 10.1590/S0100-40421998000300025 S0100-40421998000300025 S0100-40421998000300025.pdf 2998503841917815 |
dc.language.iso.fl_str_mv |
eng |
language |
eng |
dc.relation.none.fl_str_mv |
Química Nova 0.646 0,255 |
dc.rights.driver.fl_str_mv |
info:eu-repo/semantics/openAccess |
eu_rights_str_mv |
openAccess |
dc.format.none.fl_str_mv |
370-371 application/pdf |
dc.publisher.none.fl_str_mv |
Sociedade Brasileira de Química |
publisher.none.fl_str_mv |
Sociedade Brasileira de Química |
dc.source.none.fl_str_mv |
SciELO reponame:Repositório Institucional da UNESP instname:Universidade Estadual Paulista (UNESP) instacron:UNESP |
instname_str |
Universidade Estadual Paulista (UNESP) |
instacron_str |
UNESP |
institution |
UNESP |
reponame_str |
Repositório Institucional da UNESP |
collection |
Repositório Institucional da UNESP |
repository.name.fl_str_mv |
Repositório Institucional da UNESP - Universidade Estadual Paulista (UNESP) |
repository.mail.fl_str_mv |
|
_version_ |
1808129226908368896 |