QUALITY OF SAWN TIMBER DRYING OF Eucalyptus dunnii
Autor(a) principal: | |
---|---|
Data de Publicação: | 2000 |
Tipo de documento: | Artigo |
Idioma: | por |
Título da fonte: | Ciência Florestal (Online) |
DOI: | 10.5902/19805098399 |
Texto Completo: | https://periodicos.ufsm.br/cienciaflorestal/article/view/399 |
Resumo: | In the present study, the behaviour of Eucalyptus dunnii wood drying in a conventional pilot kiln was evaluated, using three drying schedules. Each drying schedule had an initial vaporization (presteaming) of 3 hours after one hour of initial warming and an intermediate vaporization of 5 hours for the collapse recovery when the wood was at 17% of humidity. The results show that among the used drying schedule only the schedule regarded as the mildest presented a good result in terms of dry wood quality. Among the discovered defects, there were 37,5% of collapse, 35% of cupping and 10% of split. Hoviever, though from this total only 15% of the collapse and cupping were regarded as strong defects. |
id |
UFSM-6_827e1230208a1b84c552d8bf7158253f |
---|---|
oai_identifier_str |
oai:ojs.pkp.sfu.ca:article/399 |
network_acronym_str |
UFSM-6 |
network_name_str |
Ciência Florestal (Online) |
spelling |
QUALITY OF SAWN TIMBER DRYING OF Eucalyptus dunniiQualidade da secagem de madeira serrada de Eucalyptus dunnii. Eucaliptus dunniipresteamingconventional drying.Eucalyptus dunnii/i>pré-vaporizaçãosecagem convencional. In the present study, the behaviour of Eucalyptus dunnii wood drying in a conventional pilot kiln was evaluated, using three drying schedules. Each drying schedule had an initial vaporization (presteaming) of 3 hours after one hour of initial warming and an intermediate vaporization of 5 hours for the collapse recovery when the wood was at 17% of humidity. The results show that among the used drying schedule only the schedule regarded as the mildest presented a good result in terms of dry wood quality. Among the discovered defects, there were 37,5% of collapse, 35% of cupping and 10% of split. Hoviever, though from this total only 15% of the collapse and cupping were regarded as strong defects. No presente estudo, foi avaliado o comportamento de secagem da madeira de Eucalyptus dunnii em estufa piloto convencional, utilizando-se três programas de secagem. Cada programa de secagem teve uma vaporização inicial (pré-vaporização) de 3 horas após uma hora de aquecimento inicial e uma vaporização intermediária de 5 horas para recuperação do colapso, quando a madeira se encontrava a 17% de umidade. Os resultados mostram que, entre os programas de secagem utilizados, somente o programa considerado o mais suave apresentou um bom resultado em termos de qualidade de madeira seca. Entre os defeitos encontrados estão 37,5% de colapso, 35% de encanoamento e 10% de rachaduras. Embora, desse total, somente 15% do colapso e encanoamento foram classificados como defeitos fortes.Universidade Federal de Santa Maria2000-03-30info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersionapplication/pdfhttps://periodicos.ufsm.br/cienciaflorestal/article/view/39910.5902/19805098399Ciência Florestal; Vol. 10 No. 1 (2000); 109-124Ciência Florestal; v. 10 n. 1 (2000); 109-1241980-50980103-9954reponame:Ciência Florestal (Online)instname:Universidade Federal de Santa Maria (UFSM)instacron:UFSMporhttps://periodicos.ufsm.br/cienciaflorestal/article/view/399/271Severo, Elias Taylor Durganteinfo:eu-repo/semantics/openAccess2017-06-07T18:29:44Zoai:ojs.pkp.sfu.ca:article/399Revistahttp://www.ufsm.br/cienciaflorestal/ONGhttps://old.scielo.br/oai/scielo-oai.php||cienciaflorestal@ufsm.br|| cienciaflorestal@gmail.com|| cf@smail.ufsm.br1980-50980103-9954opendoar:2017-06-07T18:29:44Ciência Florestal (Online) - Universidade Federal de Santa Maria (UFSM)false |
dc.title.none.fl_str_mv |
QUALITY OF SAWN TIMBER DRYING OF Eucalyptus dunnii Qualidade da secagem de madeira serrada de Eucalyptus dunnii. |
title |
QUALITY OF SAWN TIMBER DRYING OF Eucalyptus dunnii |
spellingShingle |
QUALITY OF SAWN TIMBER DRYING OF Eucalyptus dunnii QUALITY OF SAWN TIMBER DRYING OF Eucalyptus dunnii Severo, Elias Taylor Durgante Eucaliptus dunnii presteaming conventional drying. Eucalyptus dunnii /i> pré-vaporização secagem convencional. Severo, Elias Taylor Durgante Eucaliptus dunnii presteaming conventional drying. Eucalyptus dunnii /i> pré-vaporização secagem convencional. |
title_short |
QUALITY OF SAWN TIMBER DRYING OF Eucalyptus dunnii |
title_full |
QUALITY OF SAWN TIMBER DRYING OF Eucalyptus dunnii |
title_fullStr |
QUALITY OF SAWN TIMBER DRYING OF Eucalyptus dunnii QUALITY OF SAWN TIMBER DRYING OF Eucalyptus dunnii |
title_full_unstemmed |
QUALITY OF SAWN TIMBER DRYING OF Eucalyptus dunnii QUALITY OF SAWN TIMBER DRYING OF Eucalyptus dunnii |
title_sort |
QUALITY OF SAWN TIMBER DRYING OF Eucalyptus dunnii |
author |
Severo, Elias Taylor Durgante |
author_facet |
Severo, Elias Taylor Durgante Severo, Elias Taylor Durgante |
author_role |
author |
dc.contributor.author.fl_str_mv |
Severo, Elias Taylor Durgante |
dc.subject.por.fl_str_mv |
Eucaliptus dunnii presteaming conventional drying. Eucalyptus dunnii /i> pré-vaporização secagem convencional. |
topic |
Eucaliptus dunnii presteaming conventional drying. Eucalyptus dunnii /i> pré-vaporização secagem convencional. |
description |
In the present study, the behaviour of Eucalyptus dunnii wood drying in a conventional pilot kiln was evaluated, using three drying schedules. Each drying schedule had an initial vaporization (presteaming) of 3 hours after one hour of initial warming and an intermediate vaporization of 5 hours for the collapse recovery when the wood was at 17% of humidity. The results show that among the used drying schedule only the schedule regarded as the mildest presented a good result in terms of dry wood quality. Among the discovered defects, there were 37,5% of collapse, 35% of cupping and 10% of split. Hoviever, though from this total only 15% of the collapse and cupping were regarded as strong defects. |
publishDate |
2000 |
dc.date.none.fl_str_mv |
2000-03-30 |
dc.type.driver.fl_str_mv |
info:eu-repo/semantics/article info:eu-repo/semantics/publishedVersion |
format |
article |
status_str |
publishedVersion |
dc.identifier.uri.fl_str_mv |
https://periodicos.ufsm.br/cienciaflorestal/article/view/399 10.5902/19805098399 |
url |
https://periodicos.ufsm.br/cienciaflorestal/article/view/399 |
identifier_str_mv |
10.5902/19805098399 |
dc.language.iso.fl_str_mv |
por |
language |
por |
dc.relation.none.fl_str_mv |
https://periodicos.ufsm.br/cienciaflorestal/article/view/399/271 |
dc.rights.driver.fl_str_mv |
info:eu-repo/semantics/openAccess |
eu_rights_str_mv |
openAccess |
dc.format.none.fl_str_mv |
application/pdf |
dc.publisher.none.fl_str_mv |
Universidade Federal de Santa Maria |
publisher.none.fl_str_mv |
Universidade Federal de Santa Maria |
dc.source.none.fl_str_mv |
Ciência Florestal; Vol. 10 No. 1 (2000); 109-124 Ciência Florestal; v. 10 n. 1 (2000); 109-124 1980-5098 0103-9954 reponame:Ciência Florestal (Online) instname:Universidade Federal de Santa Maria (UFSM) instacron:UFSM |
instname_str |
Universidade Federal de Santa Maria (UFSM) |
instacron_str |
UFSM |
institution |
UFSM |
reponame_str |
Ciência Florestal (Online) |
collection |
Ciência Florestal (Online) |
repository.name.fl_str_mv |
Ciência Florestal (Online) - Universidade Federal de Santa Maria (UFSM) |
repository.mail.fl_str_mv |
||cienciaflorestal@ufsm.br|| cienciaflorestal@gmail.com|| cf@smail.ufsm.br |
_version_ |
1822181488047685632 |
dc.identifier.doi.none.fl_str_mv |
10.5902/19805098399 |