Luting glass ceramic restorations using a self-adhesive resin cement under different dentin conditions

Detalhes bibliográficos
Autor(a) principal: Guarda, Guilherme B
Data de Publicação: 2010
Outros Autores: Gonçalves, Luciano S, Correr, Américo B, Moraes, Rafael R, Sinhoreti, Mário A.C, Correr-Sobrinho, Lourenço
Tipo de documento: Artigo
Idioma: eng
Título da fonte: Journal of applied oral science (Online)
Texto Completo: https://www.revistas.usp.br/jaos/article/view/3790
Resumo: OBJECTIVES: The aim of this study was to investigate the bond strength of ceramic restorations luted using a self-adhesive resin cement (RelyX Unicem, 3M ESPE) under different dentin conditions. MATERIAL AND METHODS: In the experimental groups, ceramic restorations were luted to bovine incisors with RelyX Unicem under the following conditions: [Dry dentin]: surface was dried using air stream for 15 s; [Moist dentin]: excess dentin moisture was removed with absorbent paper; [Bonding agent]: Clearfil SE Bond (Kuraray) self-etching adhesive system was previously applied to dentin. In the Control group, cementation was done using an etch-and-rinse adhesive (Excite DSC) and Variolink II resin cement (Ivoclar Vivadent). Photoactivation of the resin cements was performed with UltraLume LED 5 unit (Ultradent). The restorations (n=5 per group) were sectioned into beams and microtensile testing was carried out. Data were subjected to ANOVA and Tukey's test (p
id USP-17_2d6653a25e6a3c1efa2582ca8e6afbf0
oai_identifier_str oai:revistas.usp.br:article/3790
network_acronym_str USP-17
network_name_str Journal of applied oral science (Online)
repository_id_str
spelling Luting glass ceramic restorations using a self-adhesive resin cement under different dentin conditions Dental bondingDental cementsDental porcelainTensile strength OBJECTIVES: The aim of this study was to investigate the bond strength of ceramic restorations luted using a self-adhesive resin cement (RelyX Unicem, 3M ESPE) under different dentin conditions. MATERIAL AND METHODS: In the experimental groups, ceramic restorations were luted to bovine incisors with RelyX Unicem under the following conditions: [Dry dentin]: surface was dried using air stream for 15 s; [Moist dentin]: excess dentin moisture was removed with absorbent paper; [Bonding agent]: Clearfil SE Bond (Kuraray) self-etching adhesive system was previously applied to dentin. In the Control group, cementation was done using an etch-and-rinse adhesive (Excite DSC) and Variolink II resin cement (Ivoclar Vivadent). Photoactivation of the resin cements was performed with UltraLume LED 5 unit (Ultradent). The restorations (n=5 per group) were sectioned into beams and microtensile testing was carried out. Data were subjected to ANOVA and Tukey's test (pUniversidade de São Paulo. Faculdade de Odontologia de Bauru2010-06-01info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersionapplication/pdfhttps://www.revistas.usp.br/jaos/article/view/379010.1590/S1678-77572010000300008Journal of Applied Oral Science; Vol. 18 No. 3 (2010); 244-248 Journal of Applied Oral Science; Vol. 18 Núm. 3 (2010); 244-248 Journal of Applied Oral Science; v. 18 n. 3 (2010); 244-248 1678-77651678-7757reponame:Journal of applied oral science (Online)instname:Universidade de São Paulo (USP)instacron:USPenghttps://www.revistas.usp.br/jaos/article/view/3790/4480Copyright (c) 2010 Journal of Applied Oral Scienceinfo:eu-repo/semantics/openAccessGuarda, Guilherme BGonçalves, Luciano SCorrer, Américo BMoraes, Rafael RSinhoreti, Mário A.CCorrer-Sobrinho, Lourenço2012-04-27T12:09:14Zoai:revistas.usp.br:article/3790Revistahttp://www.scielo.br/jaosPUBhttps://www.revistas.usp.br/jaos/oai||jaos@usp.br1678-77651678-7757opendoar:2012-04-27T12:09:14Journal of applied oral science (Online) - Universidade de São Paulo (USP)false
dc.title.none.fl_str_mv Luting glass ceramic restorations using a self-adhesive resin cement under different dentin conditions
title Luting glass ceramic restorations using a self-adhesive resin cement under different dentin conditions
spellingShingle Luting glass ceramic restorations using a self-adhesive resin cement under different dentin conditions
Guarda, Guilherme B
Dental bonding
Dental cements
Dental porcelain
Tensile strength
title_short Luting glass ceramic restorations using a self-adhesive resin cement under different dentin conditions
title_full Luting glass ceramic restorations using a self-adhesive resin cement under different dentin conditions
title_fullStr Luting glass ceramic restorations using a self-adhesive resin cement under different dentin conditions
title_full_unstemmed Luting glass ceramic restorations using a self-adhesive resin cement under different dentin conditions
title_sort Luting glass ceramic restorations using a self-adhesive resin cement under different dentin conditions
author Guarda, Guilherme B
author_facet Guarda, Guilherme B
Gonçalves, Luciano S
Correr, Américo B
Moraes, Rafael R
Sinhoreti, Mário A.C
Correr-Sobrinho, Lourenço
author_role author
author2 Gonçalves, Luciano S
Correr, Américo B
Moraes, Rafael R
Sinhoreti, Mário A.C
Correr-Sobrinho, Lourenço
author2_role author
author
author
author
author
dc.contributor.author.fl_str_mv Guarda, Guilherme B
Gonçalves, Luciano S
Correr, Américo B
Moraes, Rafael R
Sinhoreti, Mário A.C
Correr-Sobrinho, Lourenço
dc.subject.por.fl_str_mv Dental bonding
Dental cements
Dental porcelain
Tensile strength
topic Dental bonding
Dental cements
Dental porcelain
Tensile strength
description OBJECTIVES: The aim of this study was to investigate the bond strength of ceramic restorations luted using a self-adhesive resin cement (RelyX Unicem, 3M ESPE) under different dentin conditions. MATERIAL AND METHODS: In the experimental groups, ceramic restorations were luted to bovine incisors with RelyX Unicem under the following conditions: [Dry dentin]: surface was dried using air stream for 15 s; [Moist dentin]: excess dentin moisture was removed with absorbent paper; [Bonding agent]: Clearfil SE Bond (Kuraray) self-etching adhesive system was previously applied to dentin. In the Control group, cementation was done using an etch-and-rinse adhesive (Excite DSC) and Variolink II resin cement (Ivoclar Vivadent). Photoactivation of the resin cements was performed with UltraLume LED 5 unit (Ultradent). The restorations (n=5 per group) were sectioned into beams and microtensile testing was carried out. Data were subjected to ANOVA and Tukey's test (p
publishDate 2010
dc.date.none.fl_str_mv 2010-06-01
dc.type.driver.fl_str_mv info:eu-repo/semantics/article
info:eu-repo/semantics/publishedVersion
format article
status_str publishedVersion
dc.identifier.uri.fl_str_mv https://www.revistas.usp.br/jaos/article/view/3790
10.1590/S1678-77572010000300008
url https://www.revistas.usp.br/jaos/article/view/3790
identifier_str_mv 10.1590/S1678-77572010000300008
dc.language.iso.fl_str_mv eng
language eng
dc.relation.none.fl_str_mv https://www.revistas.usp.br/jaos/article/view/3790/4480
dc.rights.driver.fl_str_mv Copyright (c) 2010 Journal of Applied Oral Science
info:eu-repo/semantics/openAccess
rights_invalid_str_mv Copyright (c) 2010 Journal of Applied Oral Science
eu_rights_str_mv openAccess
dc.format.none.fl_str_mv application/pdf
dc.publisher.none.fl_str_mv Universidade de São Paulo. Faculdade de Odontologia de Bauru
publisher.none.fl_str_mv Universidade de São Paulo. Faculdade de Odontologia de Bauru
dc.source.none.fl_str_mv Journal of Applied Oral Science; Vol. 18 No. 3 (2010); 244-248
Journal of Applied Oral Science; Vol. 18 Núm. 3 (2010); 244-248
Journal of Applied Oral Science; v. 18 n. 3 (2010); 244-248
1678-7765
1678-7757
reponame:Journal of applied oral science (Online)
instname:Universidade de São Paulo (USP)
instacron:USP
instname_str Universidade de São Paulo (USP)
instacron_str USP
institution USP
reponame_str Journal of applied oral science (Online)
collection Journal of applied oral science (Online)
repository.name.fl_str_mv Journal of applied oral science (Online) - Universidade de São Paulo (USP)
repository.mail.fl_str_mv ||jaos@usp.br
_version_ 1800221675475697664